  1. #11
    Guest

    My civic is 8 years old and

    My civic is 8 years old and when I noticed the mileage was just not as goo,d I took it to the dealer. $3100 for a new battery. It is running fine and will do so until I get another car. Not worth replacing it. Won't buy a hybrid again and I was an ardent ecological driver. The oil change cost eat up your fuel savings. You can't take the car to a local mechanic as no one is trained on hybrids. Dealer maintenance is just too high. Looking at Jetta or Cooper now.

  2. Remove Advertisements
    HybridCars.com
    Advertisements
     

  3. #12
    Guest

    I am considering buying a

    I am considering buying a used Ford Hybrid Escape with 84,000 miles. Wondering how long these batteries last? I understand the cost to replace is $5200. Also curious on the overall maintenance of these vehicles. The benefits out way the costs. It's a moral dilemma on Earth Day. Ecology or Economy?

  4. #13
    Guest

    vw's die die die. i would

    vw's die die die.
    i would not recomend getting one if u want it long term :/

  5. #14
    Guest

    I have a '96 Accord with

    I have a '96 Accord with 322K and have not had any problems with tranny, fuel pump, etc.

  6. #15
    Guest

    They lose 20% charge


    They lose 20% charge capacity per year, as per wiki article.





    Lithium-ion battery


    From Wikipedia, the free encyclopedia

    (Redirected from Li Ion)



    Not to be confused with Lithium battery or Lithium-ion polymer battery.

    "Lithium-ion" redirects here. For the metal element, see Lithium.

    Lithium-ion battery




    Nokia Li-ion battery for powering a mobile phone



    specific energy


    100-250 Wh/kg [1]
    (0.36-0.90 MJ/kg)


    energy density


    250-620 Wh/L [2]
    (0.90-2.23 MJ/L)


    specific power

    ~250-~340 W/kg[1]



    Charge/discharge efficiency

    80-90%[3]



    Energy/consumer-price

    2.5 Wh/US$[4]



    Self-discharge rate

    8% at 21 C
    15% at 40 C
    31% at 60 C
    (per month)[5]



    Cycle durability


    400-1200 cycles
    [6]


    Nominal cell voltage

    3.6 / 3.7 V


    A lithium-ion battery (sometimes Li-ion battery or LIB) is a family of rechargeable battery types in which lithium ions move from the negative electrode to the positive electrode during discharge, and back when charging. Chemistry, performance, cost, and safety characteristics vary across LIB types. Unlike lithium primary batteries (which are disposable), lithium-ion electrochemical cells use an intercalated lithium compound as the electrode material instead of metallic lithium.

    Lithium-ion batteries are common in consumer electronics. They are one of the most popular types of rechargeable battery for portable electronics, with one of the best energy densities, no memory effect, and a slow loss of charge when not in use. Beyond consumer electronics, LIBs are also growing in popularity for military, electric vehicle, and aerospace applications.[7] Research is yielding a stream of improvements to traditional LIB technology, focusing on energy density, durability, cost, and intrinsic safety.

    Lithium-ion batteries account for 67% of all portable secondary battery sales in Japan. In the UK lithium-ion batteries account for 4.3% of all portable battery sales and in the EU 1%. [8] [9] [10]





    Contents
    [hide] 1 Charge and discharge
    2 Construction
    3 Formats
    4 History
    5 Electrochemistry 5.1 Positive electrodes
    5.2 Negative electrodes
    5.3 Electrolytes

    6 Advantages and disadvantages 6.1 Advantages
    6.2 Disadvantages 6.2.1 Cell life
    6.2.2 Internal resistance
    6.2.3 Safety requirements


    7 Specifications and design
    8 Charging procedure
    9 Variations in materials and construction
    10 Usage guidelines 10.1 Prolonging battery pack life 10.1.1 Multicell devices

    10.2 Safety 10.2.1 Recalls
    10.2.2 Transport restrictions


    11 Research
    12 See also
    13 Notes
    14 References
    15 External links


    [edit] Charge and discharge

    During discharge, lithium ions Li+ carry the current from the negative to the positive electrode, through the non-aqueous electrolyte and separator diaphragm.[11]

    During charging, an external electrical power source (the charging circuit) applies a higher voltage (but of the same polarity) than that produced by the battery, forcing the current to pass in the reverse direction. The lithium ions then migrate from the positive to the negative electrode, where they become embedded in the porous electrode material in a process known as intercalation.

    [edit] Construction





    Cylindrical 18650 cell before closing
    The three primary functional components of a lithium-ion battery are the anode, cathode, and electrolyte. The anode of a conventional lithium-ion cell is made from carbon, the cathode is a metal oxide, and the electrolyte is a lithium salt in an organic solvent.[12]

    The most commercially popular anode material is graphite. The cathode is generally one of three materials: a layered oxide (such as lithium cobalt oxide), a polyanion (such as lithium iron phosphate), or a spinel (such as lithium manganese oxide).[13]

    The electrolyte is typically a mixture of organic carbonates such as ethylene carbonate or diethyl carbonate containing complexes of lithium ions.[14] These non-aqueous electrolytes generally use non-coordinating anion salts such as lithium hexafluorophosphate (LiPF6), lithium hexafluoroarsenate monohydrate (LiAsF6), lithium perchlorate (LiClO4), lithium tetrafluoroborate (LiBF4), and lithium triflate (LiCF3SO3).

    Depending on materials choices, the voltage, capacity, life, and safety of a lithium-ion battery can change dramatically. Recently, novel architectures using nanotechnology have been employed to improve performance.

    Pure lithium is very reactive. It reacts vigorously with water to form lithium hydroxide and hydrogen gas. Thus, a non-aqueous electrolyte is typically used, and a sealed container rigidly excludes water from the battery pack.

    Lithium ion batteries are more expensive than NiCd batteries but operate over a wider temperature range with higher energy densities, while being smaller and lighter. They are fragile and so need a protective circuit to limit peak voltages.

    [edit] Formats





    Nissan Leaf's lithium-ion battery pack.
    Li-ion cells are available in various formats, which can generally be divided into four groups:[15]
    Small cylindrical (solid body without terminals, such as those used in laptop batteries)
    Large cylindrical (solid body with large threaded terminals)
    Pouch (soft, flat body, such as those used in cell phones)
    Prismatic (semi-hard plastic case with large threaded terminals, often used in vehicles' traction packs)

    The lack of case gives pouch cells the highest energy density; however, pouch cells (and prismatic cells) require an external means of containment to prevent expansion when their SOC level is high.[16]

    [edit] History





    Varta Lithium-ion battery, Museum Autovision, Altlussheim, Germany
    Lithium batteries were first proposed by M.S. Whittingham at Binghamton University, at Exxon, in the 1970s.[17] Whittingham used titanium(II) sulfide as the cathode and lithium metal as the anode.

    The reversible intercalation in graphite[18][19] and intercalation into cathodic oxides [20][21] was also already discovered in the 1970s by J.O. Besenhard at TU Munich. He also proposed the application as high energy density Lithium cells[22][23]

    Primary lithium batteries in which the anode is made from metallic lithium pose safety issues. As a result, lithium-ion batteries were developed in which both anode and cathode are made of a material containing lithium ions.

    In 1979, John Goodenough demonstrated a rechargeable cell with high cell voltage in the 4V range using lithium cobalt oxide (LiCoO2) etc. as positive electrode and Lithium metal as negative electrode.[24] This innovation provided the positive electrode material which made the lithium-ion battery (LIB) possible. LiCoO2 is a stable positive electrode material which acts as a donor of Lithium ions, which meant that it could be used with negative electrode material other than Lithium metal. By enabling the use of stable and easy-to-handle negative electrode materials, LiCoO2 opened a whole new range of possibilities for novel rechargeable battery systems.

    In 1981, Bell Labs developed a workable graphite anode[25] to provide an alternative to the lithium metal battery.

    In 1982, Rachid Yazami demonstrated the reversible electrochemical intercalation of Lithium in graphite.[26][27] The organic electrolytes available at the time would decompose during charging if used with graphite negative electrode, preventing the early development of a rechargeable battery which employed the Lithium/graphite system. Yazami used a solid electrolyte to demonstrate that Lithium could be reversibly intercalated in graphite through an electrochemical mechanism.

    In 1983, Dr. Michael Thackeray, Goodenough, and coworkers identified manganese spinel as a cathode material.[28] Spinel showed great promise, given low-cost, good electronic and lithium ion conductivity, and three-dimensional structure which gives it good structural stability. Although pure manganese spinel fades with cycling, this can be overcome with chemical modification of the material.[29] Manganese spinel is currently used in commercial cells.[30]

    In 1985, Akira Yoshino assembled a prototype cell using as anode a certain carbonaceous material into which lithium ions could be inserted and as cathode lithium cobalt oxide (LiCoO2) etc. which is stable in air.[31] By using an anode material without metallic lithium, safety was dramatically improved over batteries which used lithium metal. The use of lithium cobalt oxide (LiCoO2) enabled industrial-scale production to be achieved easily.

    This was the birth of the current lithium-ion battery.

    Then in 1991, Sony and Asahi Kasei released the first commercial lithium-ion battery.

    In 1989, Goodenough and Arumugam Manthiram of the University of Texas at Austin showed that cathodes containing polyanions, e.g. sulfates, produce higher voltages than oxides due to the inductive effect of the polyanion.[32]

    In 1996, Goodenough, Akshaya Padhi and coworkers identified lithium iron phosphate (LiFePO4) and other phospho-olivines (lithium metal phosphates with olivine structure) as cathode materials.[33]

    In 2002, Yet-Ming Chiang and his group at MIT showed a substantial improvement in the performance of lithium batteries by boosting the material's conductivity by doping it with aluminum, niobium and zirconium. The exact mechanism causing the increase became the subject of a debate.[34]

    In 2004, Chiang again increased performance by utilizing iron-phosphate particles of less than 100 nanometers in diameter. This decreased particle density by almost one hundredfold, increased the cathode's surface area and improved capacity and performance. Commercialization led to a competitive market and a patent infringement battle between Chiang and Goodenough.[34]

    [edit] Electrochemistry

    The three participants in the electrochemical reactions in a lithium-ion battery are the anode, cathode, and electrolyte.

    Both the anode and cathode are materials into which, and from which, lithium can migrate. During insertion (or intercalation) lithium moves into the electrode. During the reverse process, extraction (or deintercalation), lithium moves back out. When a lithium-based cell is discharging, the lithium is extracted from the anode and inserted into the cathode. When the cell is charging, the reverse occurs.

    Useful work can only be extracted if electrons flow through a closed external circuit. The following equations are in units of moles, making it possible to use the coefficient x.

    The positive electrode half-reaction (with charging being forwards) is: [35]



    The negative electrode half-reaction is:



    The overall reaction has its limits. Overdischarge supersaturates lithium cobalt oxide, leading to the production of lithium oxide,[36] possibly by the following irreversible reaction:



    Overcharge up to 5.2 Volts leads to the synthesis of cobalt(IV) oxide, as evidenced by x-ray diffraction[37]



    In a lithium-ion battery the lithium ions are transported to and from the cathode or anode, with the transition metal, cobalt (Co), in LixCoO2 being oxidized from Co3+ to Co4+ during charging, and reduced from Co4+ to Co3+ during discharge.

    [edit] Positive electrodes



    Electrode material

    Average potential difference

    Specific capacity

    Specific energy



    LiCoO2

    3.7 V

    140 mAh/g

    0.518 kWh/kg



    LiMn2O4

    4.0 V

    100 mAh/g

    0.400 kWh/kg



    LiNiO2

    3.5 V

    180 mAh/g

    0.630 kWh/kg



    LiFePO4

    3.3 V

    150 mAh/g

    0.495 kWh/kg



    Li2FePO4F

    3.6 V

    115 mAh/g

    0.414 kWh/kg



    LiCo1/3Ni1/3Mn1/3O2

    3.6 V

    160 mAh/g

    0.576 kWh/kg



    Li(LiaNixMnyCoz)O2

    4.2 V

    220 mAh/g

    0.920 kWh/kg


    [edit] Negative electrodes



    Electrode material

    Average potential difference

    Specific capacity

    Specific energy



    Graphite (LiC6)

    0.1-0.2 V

    372 mAh/g

    0.0372-0.0744 kWh/kg



    Hard Carbon (LiC6)

    ? V

    ? mAh/g

    ? kWh/kg



    Titanate (Li4Ti5O12)

    1-2 V

    160 mAh/g

    0.16-0.32 kWh/kg



    Si (Li4.4Si)[38]

    0.5-1 V

    4212 mAh/g

    2.106-4.212 kWh/kg



    Ge (Li4.4Ge)[39]

    0.7-1.2 V

    1624 mAh/g

    1.137-1.949 kWh/kg


    [edit] Electrolytes

    The cell voltages given in the Electrochemistry section are larger than the potential at which aqueous solutions can electrolyze, in addition lithium is highly reactive to water, therefore, nonaqueous or aprotic solutions are used.

    Liquid electrolytes in lithium-ion batteries consist of lithium salts, such as LiPF6, LiBF4 or LiClO4 in an organic solvent, such as ethylene carbonate, dimethyl carbonate, and diethyl carbonate. A liquid electrolyte conducts lithium ions, acting as a carrier between the cathode and the anode when a battery passes an electric current through an external circuit. Typical conductivities of liquid electrolyte at room temperature (20 C (68 F)) are in the range of 10 mS/cm (1 S/m), increasing by approximately 3040% at 40 C (104 F) and decreasing by a slightly smaller amount at 0 C (32 F)[40]

    Unfortunately, organic solvents easily decompose on anodes during charging. However, when appropriate organic solvents are used as the electrolyte, the solvent decomposes on initial charging and forms a solid layer called the solid electrolyte interphase (SEI),[41] which is electrically insulating yet provides sufficient ionic conductivity. The interphase prevents decomposition of the electrolyte after the second charge. For example, ethylene carbonate is decomposed at a relatively high voltage, 0.7 V vs. lithium, and forms a dense and stable interface.[citation needed]

    A good solution for the interface instability is the application of a new class of composite electrolytes based on POE (poly(oxyethylene)) developed by Syzdek et al.[42][43] It can be either solid (high molecular weight) and be applied in dry Li-polymer cells, or liquid (low molecular weight) and be applied in regular Li-ion cells.

    Another issue that Li-ion technology is facing is safety. Large scale application of Li cells in Electric Vehicles needs a dramatic decrease in the failure rate. One of the solutions is the novel technology based on reversed-phase composite electrolytes, employing porous ceramic material filled with electrolyte.[44]

    [edit] Advantages and disadvantages

    Note that both advantages and disadvantages depend on the materials and design that make up the battery. This summary reflects older designs that use carbon anode, metal oxide cathodes, and lithium salt in an organic solvent for the electrolyte.

    [edit] Advantages





    A lithium-ion battery from a laptop computer Wide variety of shapes and sizes efficiently fitting the devices they power.
    Much lighter than other energy-equivalent secondary batteries.[45]
    High open circuit voltage in comparison to aqueous batteries (such as lead acid, nickel-metal hydride and nickel-cadmium).[46] This is beneficial because it increases the amount of power that can be transferred at a lower current.
    No memory effect.
    Self-discharge rate of approximately 5-10% per month, compared to over 30% per month in common nickel metal hydride batteries, approximately 1.25% per month for Low Self-Discharge NiMH batteries and 10% per month in nickel-cadmium batteries.[47] According to one manufacturer, lithium-ion cells (and, accordingly, "dumb" lithium-ion batteries) do not have any self-discharge in the usual meaning of this word.[35] What looks like a self-discharge in these batteries is a permanent loss of capacity (see Disadvantages). On the other hand, "smart" lithium-ion batteries do self-discharge, due to the drain of the built-in voltage monitoring circuit.
    Components are environmentally safe as there is no free lithium metal.[citation needed]

    [edit] Disadvantages

    [edit] Cell life
    Charging forms deposits inside the electrolyte that inhibit ion transport. Over time, the cell's capacity diminishes. The increase in internal resistance reduces the cell's ability to deliver current. This problem is more pronounced in high-current applications. The decrease means that older batteries do not charge as much as new ones (charging time required decreases proportionally).
    High charge levels and elevated temperatures (whether from charging or ambient air) hasten capacity loss.[48][49] Charging heat is caused by the carbon anode (typically replaced with lithium titanate which drastically reduces damage from charging, including expansion and other factors).[50]
    A Standard (Cobalt) Li-ion cell that is full most of the time at 25 C (77 F) irreversibly loses approximately 20% capacity per year. Poor ventilation may increase temperatures, further shortening battery life. Loss rates vary by temperature: 6% loss at 0 C (32 F), 20% at 25 C (77 F), and 35% at 40 C (104 F). When stored at 40%60% charge level, the capacity loss is reduced to 2%, 4%, and 15%, respectively.[51][citation needed] In contrast, the calendar life of LiFePO4 cells is not affected by being kept at a high state of charge.[52]

    [edit] Internal resistance
    The internal resistance of standard (Cobalt) lithium-ion batteries is high compared to both other rechargeable chemistries such as nickel-metal hydride and nickel-cadmium, and LiFePO4 and lithium-polymer cells.[53] Internal resistance increases with both cycling and age.[49][54][55] Rising internal resistance causes the voltage at the terminals to drop under load, which reduces the maximum current draw. Eventually increasing resistance means that the battery can no longer operate for an adequate period.
    To power larger devices, such as electric cars, connecting many small batteries in a parallel circuit is more effective[56] and efficient than connecting a single large battery.[57]

    [edit] Safety requirements

    If overheated or overcharged, Li-ion batteries may suffer thermal runaway and cell rupture.[58] In extreme cases this can lead to combustion. Deep discharge may short-circuit the cell, in which case recharging would be unsafe.[59] To reduce these risks, Lithium-ion battery packs contain fail-safe circuitry that shuts down the battery when its voltage is outside the safe range of 34.2 V per cell.[35][47] When stored for long periods the small current draw of the protection circuitry itself may drain the battery below its shut down voltage; normal chargers are then ineffective. Many types of lithium-ion cell cannot be charged safely below 0C.[60]

    Other safety features are required in each cell:[35]
    shut-down separator (for overtemperature)
    tear-away tab (for internal pressure)
    vent (pressure relief)
    thermal interrupt (overcurrent/overcharging)

    These devices occupy useful space inside the cells, add additional points of failure and irreversibly disable the cell when activated. They are required because the anode produces heat during use, while the cathode may produce oxygen. These devices and improved electrode designs reduce/eliminate the risk of fire or explosion.

    These safety features increase costs compared to nickel metal hydride batteries, which require only a hydrogen/oxygen recombination device (preventing damage due to mild overcharging) and a back-up pressure valve.[47]

    [edit] Specifications and design
    Specific energy density: 150 to 250 Wh/kg (540 to 900 kJ/kg)[1]
    Volumetric energy density: 250 to 620 Wh/l (900 to 1900 J/cm)[2]
    Specific power density: 300 to 1500 W/kg (@ 20 seconds and 285 Wh/l)[1]

    Because lithium-ion batteries can have a variety of cathode and anode materials, the energy density and voltage vary accordingly.

    Lithium-ion batteries with a lithium iron phosphate cathode and graphite anode have a nominal open-circuit voltage of 3.2 V and a typical charging voltage of 3.6 V. Lithium nickel manganese cobalt (NMC) oxide cathode with graphite anodes have a 3.7 V nominal voltage with a 4.2 V max charge. The charging procedure is performed at constant voltage with current-limiting circuitry (i.e., charging with constant current until a voltage of 4.2 V is reached in the cell and continuing with a constant voltage applied until the current drops close to zero). Typically, the charge is terminated at 3% of the initial charge current. In the past, lithium-ion batteries could not be fast-charged and needed at least two hours to fully charge. Current-generation cells can be fully charged in 45 minutes or less. Some lithium-ion varieties can reach 90% in as little as 10 minutes.[61]

    [edit] Charging procedure

    Stage 1: Apply charging current until the voltage limit per cell is reached.[62]

    Stage 2: Apply maximum voltage per cell limit until the current declines below 3% of rated charge current.[62][unreliable source?]

    Stage 3: Periodically apply a top-off charge about once per 500 hours.[62][unreliable source?]

    The charge time is about three to five hours, depending on the charger used. Generally, cell phone batteries can be charged at 1C and laptop-types at 0.8C, where C is the current that would discharge the battery in one hour. Charging is usually stopped when the current goes below 0.03C but it can be left indefinitely depending on desired charging time. Some fast chargers skip stage 2 and claim the battery is ready at 70% charge.[62][unreliable source?]

    Top-off charging is recommended when voltage goes below 4.05 V/cell.[62][unreliable source?]

    Typically, lithium-ion cells are charged with 4.2 0.05 V/cell, except for military long-life cells where 3.92 V is used for extending battery life. Most protection circuits cut off if either 4.3 V or 90 C is reached. If the voltage drops below 2.50 V per cell, the battery protection circuit may also render it unchargeable with regular charging equipment. Most battery protection circuits stop at 2.73.0 V per cell.[62][unreliable source?]

    For safety reasons it is recommended the battery be kept at the manufacturer's stated voltage and current ratings during both charge and discharge cycles.

    [edit] Variations in materials and construction






    It has been suggested that Nanoball batteries be merged into this article or section. (Discuss) Proposed since September 2010.


    The increasing demand for batteries has led vendors and academics to focus on improving the power density, operating temperature, safety, durability, charging time, output power, and cost of LIB solutions.

    LIB types



    Area

    Technology

    Researchers

    Target application

    Date

    Benefit



    Cathode

    Manganese spinel (LMO)

    Lucky Goldstar Chemical,[63] NEC, Samsung,[64] Hitachi,[65] Nissan/AESC[66]

    Hybrid electric vehicle, cell phone, laptop

    1996

    durability, cost




    Lithium iron phosphate

    University of Texas/Hydro-Qubec,[67]/Phostech Lithium Inc., Valence Technology, A123Systems/MIT[68][69]

    Segway Personal Transporter, power tools, aviation products, automotive hybrid systems, PHEV conversions

    1996

    moderate density (2 Ah outputs 70 amperes) operating temperature >60 C (140 F)




    Lithium nickel manganese cobalt (NMC)

    Imara Corporation, Nissan Motor[70][71]


    2008

    density, output, safety




    LMO/NMC

    Sony, Sanyo



    power, safety (although limited durability)




    Lithium iron fluorophosphate

    University of Waterloo[72]


    2007

    durability, cost (replace Li with Na or Na/Li)




    Lithium air

    University of Dayton Research Institute[73]

    automotive

    2009

    density, safety[73]




    5% Vanadium-doped Lithium iron phosphate olivine

    Binghamton University[74]


    2008

    output



    Anode

    Lithium-titanate battery (LT)

    Altairnano

    automotive (Phoenix Motorcars), electrical grid (PJM Interconnection Regional Transmission Organization control area,[75] United States Department of Defense[76]), bus (Proterra[77])

    2008

    output, charging time, durability (20 years, 9,000 cycles), safety, operating temperature (-5070 C (-58158 F)[78][dead link]




    Lithium vanadium oxide

    Samsung/Subaru.[79]

    automotive

    2007

    density (745Wh/l)[80]




    Cobalt-oxide nano wires from genetically modified virus

    MIT


    2006

    density, thickness[81]




    Three-Dimensional (3D) Porous Particles Composed of Curved Two-Dimensional (2D) Nano-Sized Layers

    Georgia Institute of Technology [82]

    high energy batteries for electronics and electrical vehicles

    2011

    specific capacity > 2000 mAh/g, high efficiency, rapid low-cost synthesis [83]




    Iron-phosphate nano wires from genetically modified virus

    MIT


    2009

    density, thickness[84][85][86]




    Silicon/titanium dioxide composite nano wires from genetically modified tobacco virus

    University of Maryland

    explosive detection sensors, biomimetic structures, water-repellent surfaces, micro/nano scale heat pipes

    2010

    density, low charge time[87]




    Porous silicon/carbon nanocomposite spheres

    Georgia Institute of Technology

    portable electronics, electrical vehicles, electrical grid

    2010

    high stability, high capacity, low charge time[88]




    nano-sized wires on stainless steel

    Stanford University

    wireless sensors networks,

    2007

    density[89][90] (shift from anode- to cathode-limited), durability issue remains (wire cracking)




    Metal hydrides

    Laboratoire de Ractivit et de Chimie des Solides, General Motors


    2008

    density (1480 mAh/g)[91]




    Silicon Nanotubes (or Silicon Nanospheres) Confined within Rigid Carbon Outer Shells

    Georgia Institute of Technology, MSE, NanoTech Yushin's group [92]

    stable high energy batteries for cell phones, laptops, netbooks, radios, sensors and electrical vehicles

    2010

    specific capacity 2400 mAh/g, ultra-high Coulombic Efficiency and outstanding SEI stability [93]



    Electrode

    LT/LMO

    Ener1/Delphi,[94][95]


    2006

    durability, safety (limited density)




    Nanostructure

    Universit Paul Sabatier/Universit Picardie Jules Verne[96]


    2006

    density


    [edit] Usage guidelines

    [edit] Prolonging battery pack life
    Depletion below the low-voltage threshold (2.4 to 2.8 V/cell, depending on chemistry) results in a dead battery which does not even appear to charge because the protection circuit (a type of electronic fuse) disables it.[97] This can be reversed in many modern batteries, especially single-cell ones, by applying a charging voltage for long enough to make the cell voltage rise above the low-voltage threshold; however this behaviour varies by manufacturer.
    Lithium-ion batteries should be kept cool; they may be stored in a refrigerator.[97][98]
    The rate of degradation of Lithium-ion batteries is strongly temperature-dependent; they degrade much faster if stored or used at higher temperatures.[97][99]
    The rate of degradation of Lithium-ion batteries is also related to battery charge level; they degrade much faster when at 100% charge, than at lower charges. Since batteries die if deep discharged (depleted) and since a battery has some self-discharge it is frequently recommended to store batteries at 40% charge level. [100]

    [edit] Multicell devices

    Li-ion batteries require a Battery Management System to prevent operation outside each cell's Safe Operating Area (over-charge, under-charge, safe temperature range) and to balance cells to eliminate SOC mismatches, significantly improving battery efficiency and increasing overall capacity.[101] As the number of cells and load currents increase, the potential for mismatch also increases.[102] There are two kinds of mismatch in the pack: state-of-charge (SOC) and capacity/energy ("C/E") mismatch. Though SOC is more common, each problem limits pack capacity (mAh) to the capacity of the weakest cell.

    [edit] Safety

    Lithium-ion batteries can rupture, ignite, or explode when exposed to high temperature. Short-circuiting a battery will cause the cell to overheat and possibly to catch fire. Adjacent cells may also then heat up and fail, in some cases, causing the entire battery to ignite or rupture. In the event of a fire, the device may emit dense irritating smoke.[103]

    Replacing the lithium cobalt oxide cathode material in lithium-ion batteries with a lithium metal phosphate such as lithium iron phosphate, improves cycle counts, shelf life and safety, but lowers capacity. Currently, these 'safer' lithium-ion batteries are mainly used in electric cars and other large-capacity battery applications, where safety issues are critical.[104]

    Lithium-ion batteries normally contain safety devices to protect the cells from disturbance. However, contaminants inside the cells can defeat these safety devices.

    [edit] Recalls

    In March 2007, Lenovo recalled approximately 205,000 batteries at risk of explosion. In August 2007, Nokia recalled over 46 million batteries at risk of overheating and exploding.[105] One such incident occurred in the Philippines involving a Nokia N91, which uses the BL-5C battery.[106]

    In December 2006, Dell recalled approximately 22,000 laptop batteries from the U.S. market.[107] Approximately 10 million Sony batteries used in Dell, Sony, Apple, Lenovo/IBM, Panasonic, Toshiba, Hitachi, Fujitsu and Sharp laptops were recalled in 2006. The batteries were found to be susceptible to internal contamination by metal particles. Under some circumstances, these particles could pierce the separator, causing a short-circuit.[108]

    In October 2004, Kyocera Wireless recalled approximately 1 million mobile phone batteries to identify counterfeits.[109]

    [edit] Transport restrictions

    In January 2008, the United States Department of Transportation ruled that passengers on board commercial aircraft could carry lithium batteries in their checked baggage if the batteries are installed in a device. Types of batteries affected by this rule are those containing lithium, including Li-ion, lithium polymer, and lithium cobalt oxide chemistries. Lithium-ion batteries containing more than 25 grams (0.88 oz) equivalent lithium content (ELC) are exempt from the rule and are forbidden in air travel.[110] This restriction greatly reduces the chances of the batteries short-circuiting and causing a fire.[citation needed]

    Additionally, a limited number of replacement batteries may be transported in carry-on luggage. Such batteries must be sealed in their original protective packaging or in individual containers or plastic bags.[110][111]

    Some postal administrations restrict air shipping (including EMS) of lithium and lithium-ion batteries, and products containing these (e.g. laptops, cell phones etc.). Among these countries and regions are Hong Kong,[112] Australia and Japan.[113]

    [edit] Research

    Researchers are working to improve the power density, safety, recharge cycle, cost and other characteristics of these batteries.

    Solid-state designs have the potential to deliver three times the energy density of typical 2011 lithium-ion batteries at less than half the cost per kilowatt-hour. This approach eliminates binders, separators, and liquid electrolytes. By eliminating these, "you can get around 95% of the theoretical energy density of the active materials."[114]

    Earlier trials of this technology ran into cost barriers, because the semiconductor industry's vacuum deposition technology cost 2030 times too much. The new process deposits semiconductor-quality films from a solution. The nanostructured films grow directly on a substrate and then sequentially on top of each other. The process allows the firm to "spray-paint a cathode, then a separator/electrolyte, then the anode. It can be cut and stacked in various form factors."[114]

    [edit] See also





    Book: Lithium-ion batteries



    Wikipedia Books are collections of articles that can be downloaded or ordered in print.

    Potassium-ion battery
    Nanowire battery




    [edit] Notes

    1.^ a b c d "Rechargeable Li-Ion OEM Battery Products". Panasonic.com. Retrieved 2010-04-23.
    2.^ a b "Panasonic Develops New Higher-Capacity 18650 Li-Ion Cells; Application of Silicon-based Alloy in Anode". greencarcongress.com. Retrieved 2011-01-31.
    3.^ Valen & Shoesmith (2007). The effect of PHEV and HEV duty cycles on battery and battery pack performance (PDF). 2007 Plug-in Highway Electric Vehicle Conference: Proceedings. Retrieved 2010-06-11.
    4.^ 11.10V,6600Mah, Li-Ion, Replacement Laptop Battery For Dell (etc). Amazon.com Online Store. Retrieved 2010-06-11.
    5.^ H. Abea, T. Muraia and K. Zaghibb (1999). Vapor-grown carbon fiber anode for cylindrical lithium ion rechargeable batteries. Journal of Power Sources 77:2, February 1999, pp. 110-115. DOI:10.1016/S0378-7753(98)00158-X. Retrieved 2010-06-11.
    6.^ Battery Types and Characteristics for HEV ThermoAnalytics, Inc., 2007. Retrieved 2010-06-11.
    7.^ Ballon, Massie Santos (14 October 2008). "Electrovaya, Tata Motors to make electric Indica". cleantech.com. Cleantech Group. Retrieved 2010-06-11.
    8.^ [1] Monthly battery sales statistics - MoETI - March 2011
    9.^ [2] Battery Waste Management - 2006 DEFRA
    10.^ [3] EPBA statistics - 2000
    11.^ David Linden, Thomas B. Reddy (ed). Handbook Of Batteries 3rd Edition. McGraw-Hill, New York, 2002 ISBN 0-07-135978-8 chapter 35
    12.^ Silberberg, M. 2006. Chemistry: The Molecular Nature of Matter and Change, 4th Ed. New York (NY): McGraw-Hill Education. p 935.
    13.^ Thackeray, Thomas, and Whittingham (March 2000). Science and Applications of Mixed Conductors for Lithium Batteries. mrs.com; Materials Research Society. Retrieved 2010-06-11.
    14.^ MSDS: National Power Corp Lithium Ion Batteries (PDF). tek.com; Tektronix Inc., 7 May 2004. Retrieved 2010-06-11.
    15.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 2
    16.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 234
    17.^ M Stanley Whittingham. Electrical Energy Storage and Intercalation Chemistry Science: 192 (4244): 1126
    18.^ J.O.Besenhard and H.P. Fritz, Cathodic Reduction of Graphite in Organic Solutions of Alkali and NR 4+ Salts, J. Electroanal. Chem., 53, 329 (1974)
    19.^ J.O. Besenhard, The Electrochemical Preparation and Properties of Ionic Alkali Metal and NR 4+ Graphite Intercalation Compounds in Organic Electrolytes, Carbon, 14, 111 (1976)
    20.^ R. Schallhorn, R. Kuhlmann, and J.O. Besenhard, Topotactic Redox Reactions and Ion Exchange of Layered MoO3 Bronzes,, Mat. Res. Bull., 11, 83 (1976)
    21.^ J.O. Besenhard and R. Schallhorn, The Discharge Reaction Mechanism of the MoO3 Electrode in Organic Electrolytes J. Power Sources, 1, 267 (1976/77)
    22.^ J.O. Besenhard and G. Eichinger, High Energy Density Lithium Cells. Part I. Electrolytes and Anodes, J. Electroanal. Chem., 68, 1 (1976); and G. Eichinger
    23.^ J.O. Besenhard, High Energy Density Lithium Cells. Part II. Cathodes and Complete Cells, J. Electroanal. Chem., 72, 1 (1976)
    24.^ USPTO search for inventions by "Goodenough, John"
    25.^ US 4304825, Basu; Samar, "Rechargeable battery", issued 8 December 1981, assigned to Bell Telephone Laboratories
    26.^ International Meeting on Lithium Batteries, Rome, April 2729, 1982, C.L.U.P. Ed. Milan, Abstract #23
    27.^ Journal of Power Sources (AprilMay 1983), 9 (34), 365371
    28.^ M.M. Thackeray, W.I.F. David, P.G. Bruce, and J.B. Goodenough (4 February 1983). "Lithium insertion into manganese spinels". Materials Research Bulletin (Elsevier) 18 (4): 461472. doi:10.1016/0025-5408(83)90138-1.
    29.^ Gholamabbas Nazri, Gianfranco Pistoia (2004). Lithium batteries: science and ... - Google Books. Springer. ISBN 9781402076282. Retrieved 2009-10-08.
    30.^ Voelcker, John (September 2007). Lithium Batteries Take to the Road IEEE Spectrum.
    31.^ US 4668595, Yoshino; Akira, "Secondary Battery", issued 10 May 1985, assigned to Asahi Kasei
    32.^ A. Manthiram and J.B. Goodenough Corresponding (16 May 1989). "Lithium insertion into Fe2(SO4)3 frameworks". Journal of Power Sources (Elsevier B.V.) 26 (3-4): 403408. doi:10.1016/0378-7753(89)80153-3.
    33.^ "Phospho-olivines as positive-electrode materials for rechargeable lithium batteries". Electrochem. Society 144: 11881194. 1997.
    34.^ a b Editors (6 March 2008). "In search of the perfect battery" (PDF). The Economist. Archived from the original on 2009-09-25. Retrieved 2010-05-11.
    35.^ a b c d Staff (November 2003) (PDF). Lithium Ion technical handbook. Gold Peak Industries Ltd..
    36.^ H.C. Choi et al., J. Phys. Chem. B 107 p5806(2003) doi:10.1021/jp030438w
    37.^ G.G. Amatucci, J.M. Tarascon, L.C. Kein J. Electrochemical Society 143 p1114 1996 doi:10.1149/1.1836594
    38.^ R. Ruffo; S. S. Hong, C. K. Chan, R. A. Huggins, Y. Cui (2009). "Impedance Analysis of Silicon Nanowire Lithium Ion Battery Anodes" (PDF). J. Phys. Chem. C. 113 (113 (26), (2009)): 1139011398. doi:10.1021/jp901594g. Retrieved 2009-09-01.
    39.^ C. K. Chan; X. F. Zhang, Y. Cui (2007). "High Capacity Li-ion Battery Anodes Using Ge Nanowires" (PDF). Nano Lett. 8 (8 (2007)): 307309. Bibcode 2008NanoL...8..307C. doi:10.1021/nl0727157. PMID 18095738.
    40.^ Wenige, Niemann, et al. (May 30, 1998). Liquid Electrolyte Systems for Advanced Lithium Batteries (PDF). cheric.org; Chemical Engineering Research Information Center(KR). Retrieved 2010-06-11.
    41.^ Balbuena, P.B., Wang, Y.X., eds. Lithium Ion Batteries: Solid Electrolyte Interphase 2004 Imperial College Press, London
    42.^ Syzdek, Jaroslaw, et al., Journal of Power Sources, 173, 2007, p712-720 doi:10.1016/j.jpowsour.2007.05.061
    43.^ Syzdek, Jaroslaw, et al., Electrochimica Acta, 55, 2010, p1314-1322, doi:10.1016/j.electacta.2009.04.025
    44.^ Syzdek, Jaroslaw, et al., Journal of Power Sources, 194, 2009, p66-72, doi:10.1016/j.jpowsour.2009.01.070
    45.^ Winter & Brodd 2004, pp. 4256, 4258
    46.^ , Winter & Brodd 2004, p. 4254
    47.^ a b c Winter & Brodd 2004, p. 4259
    48.^ Aging - capacity loss BatteryUniversity.com.[unreliable source?]
    49.^ a b Winter & Brodd 2004, p. 4258
    50.^ Altair Nano: Power & Energy Systems[dead link]
    51.^ . Battery University: Fig. 1 Non-recoverable capacity loss[unreliable source?]
    52.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 9
    53.^ "A123 M1 cell specifications".
    54.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 12
    55.^ Buchmann, Isidor (200804). "Choosing a battery that will last". Isidor Buchmann (CEO of Cadex Electronics Inc.).[unreliable source?]
    56.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 229
    57.^ Buchmann, Isidor (September 2006). "BatteryUniversity.com: How to prolong lithium-based batteries". Cadex Electronics Inc..[unreliable source?]
    58.^ Spotnitz, R.; Franklin, J. (2003). "Abuse behavior of high-power, lithium-ion cells". Journal of Power Sources (Elsevier) 113: 81100. doi:10.1016/S0378-7753(02)00488-3.
    59.^ Buchmann, Isidor (February 2003). "Advanced battery analyzers". Isidor Buchmann. Retrieved 2009-12-26.[unreliable source?]
    60.^ "Lithium-ion Battery Charging Basics". PowerStream Technologies. Retrieved 4 December 2010.
    61.^ AeroVironment achieves electric vehicle fast-charge milestone avinc.com; AeroVironment, 30 May 2007. (Press release). "Test rapidly recharges a battery pack designed for use in passenger vehicles. 10-minute recharge restores enough energy to run electric vehicle for two hours at 60 miles per hour."
    62.^ a b c d e f "Charging lithium-ion batteries". batteryuniversity.com. Retrieved 2009-05-21.[unreliable source?]
    63.^ Kevin Jost [ed.] (October 2006). Tech Briefs: CPI takes new direction on Li-ion batteries (PDF). aeionline.org; Automotive Engineering Online. Archived from the original. Retrieved 2010-06-11.
    64.^ Voelcker, John (September 2007). Lithium Batteries Take to the Road. IEEE Spectrum. Retrieved 2010-06-15.
    65.^ Loveday, Eric (23 April 2010). "Hitachi develops new manganese cathode, could double life of li-ion batteries". Retrieved 2010-06-11..
    66.^ Nikkei (29 November 2009). Report: Nissan On Track with Nickel Manganese Cobalt Li-ion Cell for Deployment in 2015 Green Car Congress (blog). Retrieved 2010-06-11.
    67.^ Elder, Robert and Zehr, Dan (16 February 2006). Valence sued over UT patent Austin American-Statesman (courtesy Bickle & Brewer Law Firm). Archived from the original. Retrieved 2010-06-11.
    68.^ Bulkeley, William M. (26 November 2005). "New Type of Battery Offers Voltage Aplenty, at a Premium". The Day: p. E6.
    69.^ A123Systems (2 November 2005). A123Systems Launches New Higher-Power, Faster Recharging Li-Ion Battery Systems Green Car Congress; A123Systems (Press release). Retrieved 2010-05-11.
    70.^ Imara Corporation website
    71.^ O'Dell, John (17 December 2008). Fledgling Battery Company Says Its Technology Boosts Hybrid Battery Performance Green Car Advisor; Edmunds Inc. Retrieved 2010-06-11.
    72.^ B. L. Ellis, W. R. M. Makahnouk, Y. Makimura, K. Toghill & L. F. Nazar (9 September 2007). A multifunctional 3.5 V iron-based phosphate cathode for rechargeable batteries. 6. Nature Materials. pp. 749753. Bibcode 2007NatMa...6..749E. doi:10.1038/nmat2007. Retrieved 2009-10-08.
    73.^ a b "A Research First: Lithium Air Battery Development (Press Release)". 17 November 2009. Retrieved 2010-06-11.
    74.^ Jian Hong, C. S. Wang, Shailesh Upreti and M. Stanley Whittinghama. "Vanadium Modified LiFePO4 Cathode for Li-ion Batteries". ECS (ETS) 12 (2): A33. Retrieved 2010-06-11.
    75.^ Altair Nanotechnologies (21 November 2008). "... Acceptance of the First Grid-Scale, Battery Energy Storage System". Press release. Retrieved 2009-10-08.
    76.^ Marty Ozols (11 November 2009). Altair Nanotechnologies Power Partner - The Military Systemagicmotives (personal webpage)[dubious discuss]. Retrieved 2010-06-11.
    77.^ "Proterra Corporate website". Proterra. Retrieved 2009-10-08.[dead link]
    78.^ Microsoft PowerPoint - 061125 Altair EDTA Presentation
    79.^ Blain, Loz (2 November 2007). "Subaru doubles the battery range on its electric car concept". gizmag. Retrieved 2009-10-08.
    80.^ "Li-Ion Rechargeable Batteries Made Safer". Nikkei Electronics Asia. 29 January 2008. Retrieved 2009-10-08.
    81.^ Ki Tae Nam, Dong-Wan Kim, et. al. (6 April 2006). Virus-Enabled Synthesis and Assembly of Nanowires for Lithium Ion Battery Electrodes. Science Express (preprint). Retrieved 2010-06-11.(subscription required)
    82.^ "gatech.edu".
    83.^ Kara Evanoff, Alexandre Magasinskiy, Junbing Yang and Gleb Yushin (April 21, 2011). "Nanosilicon-Coated Graphene Granules as Anodes for Li-Ion Batteries". Advanced Energy Materials. doi:10.1002/aenm.201100071. Retrieved 2011-04-21.
    84.^ Palca, Joe (6 April 2009). Hidden Ingredient In New, Greener Battery: A Virus. npr.org; National Public Radio. Retrieved 2010-06-11.
    85.^ Zandonella, Catherine (11 April 2009). "Battery grown from "armour plated" viruses". New Scientist (Tribune media Services International) 202 (2703): 1.
    86.^ Bullis, Kevin (28 September 2006). "Powerful Batteries That Assemble Themselves". technologyreview.com. Technology Review. Retrieved 2010-06-15.
    87.^ "Bad Virus Put to Good Use". Clark School of Engineering, University of Maryland. December 6, 2010. Retrieved December, 2010.
    88.^ "Self-Assembled Nanocomposites Boost Lithium-Ion Battery Anodes". Nature Materials and Georgia Institute of Technology. March 15, 2010. Retrieved March, 2010.
    89.^ "New Nanowire Battery Holds 10 Times The Charge Of Existing Ones". sciencedaily.com. Science Daily. 20 December 2007.
    90.^ Dennis, Lyle (21 December 2007). "Interview with Dr. Cui, Inventor of Silicon Nanowire Lithium-ion Battery Breakthrough". GM-Volt. Retrieved 2009-10-08.
    91.^ Y. Oumellal, A. Rougier, G. A. Nazri, J-M. Tarascon & L. Aymard (12 October 2008). "Metal hydrides for lithium-ion batteries". Nature Materials 7 (11): 916921. Bibcode 2008NatMa...7..916O. doi:10.1038/nmat2288. Retrieved 2009-10-08.
    92.^ "Error: no |title= specified when using {{Cite web}}". http://www.nano-tech.gatech.edu/.
    93.^ Benjamin Hertzberg, Alexander Alexeev and Gleb Yushin (June 8, 2010). "Deformations in Si?Li Anodes Upon Electrochemical Alloying in Nano-Confined Space". JACS 132 (25): 85488549. doi:10.1021/ja1031997. Retrieved 2010-06-08.
    94.^ Welcome to Ener1. Ener1 (Press release). Archived from the original 2006-07-08. Retrieved 2010-06-11.
    95.^ EnerDel Technical Presentation (PDF). EnerDel Corporation. 29 October 2007. Archived from the original. Retrieved 2010-06-11.
    96.^ Bullis, Kevin (22 June 2006). Higher-Capacity Lithium-Ion Batteries Technology Review. Retrieved 2010-06-11.
    97.^ a b c http://batteryuniversity.com/parttwo-34.htm
    98.^ L.M. Cristo, T. B. Atwater. Characteristics and Behavior of 1M LiPF6 1EC:1DMC Electrolyte at Low Temperatures. Fort Monmouth, NJ: U.S. Army Research.
    99.^ Modelling capacity fade in Lithium-ion cells, Bor Yann Liaw, Jungst, Nagasubramanian, and Doughty, Sandia National Laboratory
    100.^ batteryuniversity.com: How to Prolong Lithium-based Batteries, Research is performed by the Center for Automotive Research at the Ohio State University in collaboration with Oak Ridge National Laboratory and the National Institute of Standards Technology
    101.^ Andrea, Davide (21 August 2008). About Battery Management Systems. ELithion LLC. Retrieved 2010-06-15.
    102.^ Andrea, Davide (19 September 2008). White Paper - CCCV chargers: a false sense of security. ELithion LLC. Retrieved 2010-06-15.
    103.^ Electrochem Commercial Power (9 September 2006). "Safety and handling guidelines for Electrochem Lithium Batteries" (PDF). http://marine.rutgers.edu. Rutgers University. Retrieved 2009-05-21.
    104.^ Cringely, Robert X. (1 September 2006). "Safety Last". The New York Times. Retrieved 2010-04-14.
    105.^ Nokia issues BL-5C battery warning, offers replacement. Wikinews. 14 August 2007. Retrieved 2009-10-08.
    106.^ Staff (27 July 2007). Nokia N91 cell phone explodes Mukamo - Filipino News (blog). Retrieved 2010-06-15.
    107.^ Tullo, Alex. (21 August 2006). "Dell Recalls Lithium Batteries". Chemical and Engineering News:11; American Chemical Society. Retrieved 2010-06-15.
    108.^ Hales, Paul (21 June 2006). Dell laptop explodes at Japanese conference. The Inquirer. Retrieved 2010-06-15.
    109.^ Kyocera Wireless (28 October 2004). "Kyocera Launches Precautionary Battery Recall, Pursues Supplier of Counterfeit Batteries". Press release. Archived from the original on 7 January 2006. Retrieved 2010-06-15.
    110.^ a b "Safe Travel". Safetravel.dot.gov. U.S. Department of Transportation. 1 January 2008. Retrieved 2009-10-08.
    111.^ Galbraith, Rob (3 January 2008). "U.S. Department of Transportation revises lithium battery rules press release". Little Guy Media. Retrieved 2009-05-11.
    112.^ Prohibitions - 6.3.12 - Dangerous, offensive and indecent articles (PDF). Hong Kong Post Office Guide. December 2009. Retrieved 2010-06-15.
    113.^ International Mail > FAQs > Goods/Services: Shipping a Laptop Japan Post Service Co. Ltd. Retrieved 2010-06-15.
    114.^ a b Melody Voth (December 6, 2010). "Battery Booster". Retrieved February 9, 2011.

    [edit] References

    Winter, M.; Brodd, J. (2004). "What Are Batteries, Fuel Cells, and Supercapacitors?" (PDF). Chemical Review 104 (104): 4245. doi:10.1021/cr020730k. Retrieved 2010-07-25.

    [edit] External links





    Wikimedia Commons has media related to: Lithium-ion batteries

    Asahi Kasei Corporation -- Father of the lithium-ion battery
    Lithium batteries at the Open Directory Project
    Argonne opens chapter in battery research -- lithium air. Argonne National Labs. Press release. 14 September 2009.
    Battery and Energy Technologies - Rechargeable Lithium batteries. Electropaedia; Woodbank Communications Ltd. Updated 28 April 2010.
    Stanford's nanowire battery holds 10 times the charge of existing ones. Stanford Report, 18 December 2007. Press release.
    The Lithium Ion Battery. E-Articles.com. (Self-publishing site).
    The Future of Electric Vehicles: Setting the Record Straight on Lithium Availability. Journal of Energy Security, 27 August 2009. Keith Evans.
    Researchers from Spheric Technologies and Arizona State University Describe Major Advances in the Use of Microwaves to Produce Key Lithium Ion Battery Materials; Present Papers at MS&T'10 Conference, October 17-21. Spheric Technologies. Press release. October 18, 2010.






    [hide]v d eGalvanic cells






    Non-rechargeable:
    primary cells


    Alkaline battery Aluminium battery Bunsen cell Chromic acid cell Clark cell Daniell cell Dry cell Grove cell Leclanch cell Lithium battery Mercury battery Nickel oxyhydroxide battery Silver-oxide battery Weston cell Zamboni pile Zincair battery Zinccarbon battery Zincchloride battery








    Rechargeable:
    secondary cells


    Automotive battery Leadacid battery Lead-acid battery (gel) Lithium air battery Lithium-ion battery Beltway battery Lithium-ion polymer battery Lithium iron phosphate battery Lithium sulfur battery Lithium-titanate battery Nickel-cadmium battery Nickel hydrogen battery Nickel-iron battery Nickel-lithium battery Nickel-metal hydride battery Low self-discharge NiMH battery Nickel-zinc battery Potassium-ion battery Rechargeable alkaline battery Silicon air battery Sodium-ion battery Sodium-sulfur battery Vanadium redox battery Zinc-bromine battery Zinc-cerium battery






    Kinds of cells


    Battery (including Wet cell Dry cell) Concentration cell Flow battery Fuel cell Trough battery Voltaic pile






    Parts of cells


    Anode Catalyst Cathode Electrolyte Half cell Ions Salt bridge Semipermeable membrane








    View page ratings



    Rate this page



    What's this?






    Trustworthy
















    Objective
















    Complete
















    Well-written

















    I am highly knowledgeable about this topic (optional)












    Submit ratings













































    Categories: Lithium-ion batteries | Rechargeable batteries | Metal-ion batteries | Product recalls | Product safety scandals







    Log in / create account




    Article
    Discussion








    Read
    Edit
    View history

















    Main page
    Contents
    Featured content
    Current events
    Random article
    Donate to Wikipedia


    Interaction

    Help
    About Wikipedia
    Community portal
    Recent changes
    Contact Wikipedia


    Toolbox










    Print/export






    Languages

    ???????
    ?????????
    Catal
    ?esky
    Dansk
    Deutsch
    Eesti
    Espaol
    Esperanto
    ?????
    Franais
    ???
    Italiano
    Magyar
    ??????
    Nederlands
    ???
    ?Norsk (bokml)?
    Polski
    Portugus
    Romn?
    ???????
    Simple English
    Suomi
    Svenska
    Trke
    ??????????
    ??

    This page was last modified on 27 July 2011 at 11:51.

    Text is available under the Creative Commons Attribution-ShareAlike License; additional terms may apply. See Terms of use for details.
    Wikipedia is a registered trademark of the Wikimedia Foundation, Inc., a non-profit organization.

    Contact us
    Privacy policy
    About Wikipedia
    Disclaimers





  7. #16
    Guest

    They lose 20% charge


    They lose 20% charge capacity per year, as per wiki article.
    I'm asuming this means over time the gasoline engine is used more often reducing efficiency over time.




    Lithium-ion battery


    From Wikipedia, the free encyclopedia

    (Redirected from Li Ion)



    Not to be confused with Lithium battery or Lithium-ion polymer battery.

    "Lithium-ion" redirects here. For the metal element, see Lithium.

    Lithium-ion battery




    Nokia Li-ion battery for powering a mobile phone



    specific energy


    100-250 Wh/kg [1]
    (0.36-0.90 MJ/kg)


    energy density


    250-620 Wh/L [2]
    (0.90-2.23 MJ/L)


    specific power

    ~250-~340 W/kg[1]



    Charge/discharge efficiency

    80-90%[3]



    Energy/consumer-price

    2.5 Wh/US$[4]



    Self-discharge rate

    8% at 21 C
    15% at 40 C
    31% at 60 C
    (per month)[5]



    Cycle durability


    400-1200 cycles
    [6]


    Nominal cell voltage

    3.6 / 3.7 V


    A lithium-ion battery (sometimes Li-ion battery or LIB) is a family of rechargeable battery types in which lithium ions move from the negative electrode to the positive electrode during discharge, and back when charging. Chemistry, performance, cost, and safety characteristics vary across LIB types. Unlike lithium primary batteries (which are disposable), lithium-ion electrochemical cells use an intercalated lithium compound as the electrode material instead of metallic lithium.

    Lithium-ion batteries are common in consumer electronics. They are one of the most popular types of rechargeable battery for portable electronics, with one of the best energy densities, no memory effect, and a slow loss of charge when not in use. Beyond consumer electronics, LIBs are also growing in popularity for military, electric vehicle, and aerospace applications.[7] Research is yielding a stream of improvements to traditional LIB technology, focusing on energy density, durability, cost, and intrinsic safety.

    Lithium-ion batteries account for 67% of all portable secondary battery sales in Japan. In the UK lithium-ion batteries account for 4.3% of all portable battery sales and in the EU 1%. [8] [9] [10]





    Contents
    [hide] 1 Charge and discharge
    2 Construction
    3 Formats
    4 History
    5 Electrochemistry 5.1 Positive electrodes
    5.2 Negative electrodes
    5.3 Electrolytes

    6 Advantages and disadvantages 6.1 Advantages
    6.2 Disadvantages 6.2.1 Cell life
    6.2.2 Internal resistance
    6.2.3 Safety requirements


    7 Specifications and design
    8 Charging procedure
    9 Variations in materials and construction
    10 Usage guidelines 10.1 Prolonging battery pack life 10.1.1 Multicell devices

    10.2 Safety 10.2.1 Recalls
    10.2.2 Transport restrictions


    11 Research
    12 See also
    13 Notes
    14 References
    15 External links


    [edit] Charge and discharge

    During discharge, lithium ions Li+ carry the current from the negative to the positive electrode, through the non-aqueous electrolyte and separator diaphragm.[11]

    During charging, an external electrical power source (the charging circuit) applies a higher voltage (but of the same polarity) than that produced by the battery, forcing the current to pass in the reverse direction. The lithium ions then migrate from the positive to the negative electrode, where they become embedded in the porous electrode material in a process known as intercalation.

    [edit] Construction





    Cylindrical 18650 cell before closing
    The three primary functional components of a lithium-ion battery are the anode, cathode, and electrolyte. The anode of a conventional lithium-ion cell is made from carbon, the cathode is a metal oxide, and the electrolyte is a lithium salt in an organic solvent.[12]

    The most commercially popular anode material is graphite. The cathode is generally one of three materials: a layered oxide (such as lithium cobalt oxide), a polyanion (such as lithium iron phosphate), or a spinel (such as lithium manganese oxide).[13]

    The electrolyte is typically a mixture of organic carbonates such as ethylene carbonate or diethyl carbonate containing complexes of lithium ions.[14] These non-aqueous electrolytes generally use non-coordinating anion salts such as lithium hexafluorophosphate (LiPF6), lithium hexafluoroarsenate monohydrate (LiAsF6), lithium perchlorate (LiClO4), lithium tetrafluoroborate (LiBF4), and lithium triflate (LiCF3SO3).

    Depending on materials choices, the voltage, capacity, life, and safety of a lithium-ion battery can change dramatically. Recently, novel architectures using nanotechnology have been employed to improve performance.

    Pure lithium is very reactive. It reacts vigorously with water to form lithium hydroxide and hydrogen gas. Thus, a non-aqueous electrolyte is typically used, and a sealed container rigidly excludes water from the battery pack.

    Lithium ion batteries are more expensive than NiCd batteries but operate over a wider temperature range with higher energy densities, while being smaller and lighter. They are fragile and so need a protective circuit to limit peak voltages.

    [edit] Formats





    Nissan Leaf's lithium-ion battery pack.
    Li-ion cells are available in various formats, which can generally be divided into four groups:[15]
    Small cylindrical (solid body without terminals, such as those used in laptop batteries)
    Large cylindrical (solid body with large threaded terminals)
    Pouch (soft, flat body, such as those used in cell phones)
    Prismatic (semi-hard plastic case with large threaded terminals, often used in vehicles' traction packs)

    The lack of case gives pouch cells the highest energy density; however, pouch cells (and prismatic cells) require an external means of containment to prevent expansion when their SOC level is high.[16]

    [edit] History





    Varta Lithium-ion battery, Museum Autovision, Altlussheim, Germany
    Lithium batteries were first proposed by M.S. Whittingham at Binghamton University, at Exxon, in the 1970s.[17] Whittingham used titanium(II) sulfide as the cathode and lithium metal as the anode.

    The reversible intercalation in graphite[18][19] and intercalation into cathodic oxides [20][21] was also already discovered in the 1970s by J.O. Besenhard at TU Munich. He also proposed the application as high energy density Lithium cells[22][23]

    Primary lithium batteries in which the anode is made from metallic lithium pose safety issues. As a result, lithium-ion batteries were developed in which both anode and cathode are made of a material containing lithium ions.

    In 1979, John Goodenough demonstrated a rechargeable cell with high cell voltage in the 4V range using lithium cobalt oxide (LiCoO2) etc. as positive electrode and Lithium metal as negative electrode.[24] This innovation provided the positive electrode material which made the lithium-ion battery (LIB) possible. LiCoO2 is a stable positive electrode material which acts as a donor of Lithium ions, which meant that it could be used with negative electrode material other than Lithium metal. By enabling the use of stable and easy-to-handle negative electrode materials, LiCoO2 opened a whole new range of possibilities for novel rechargeable battery systems.

    In 1981, Bell Labs developed a workable graphite anode[25] to provide an alternative to the lithium metal battery.

    In 1982, Rachid Yazami demonstrated the reversible electrochemical intercalation of Lithium in graphite.[26][27] The organic electrolytes available at the time would decompose during charging if used with graphite negative electrode, preventing the early development of a rechargeable battery which employed the Lithium/graphite system. Yazami used a solid electrolyte to demonstrate that Lithium could be reversibly intercalated in graphite through an electrochemical mechanism.

    In 1983, Dr. Michael Thackeray, Goodenough, and coworkers identified manganese spinel as a cathode material.[28] Spinel showed great promise, given low-cost, good electronic and lithium ion conductivity, and three-dimensional structure which gives it good structural stability. Although pure manganese spinel fades with cycling, this can be overcome with chemical modification of the material.[29] Manganese spinel is currently used in commercial cells.[30]

    In 1985, Akira Yoshino assembled a prototype cell using as anode a certain carbonaceous material into which lithium ions could be inserted and as cathode lithium cobalt oxide (LiCoO2) etc. which is stable in air.[31] By using an anode material without metallic lithium, safety was dramatically improved over batteries which used lithium metal. The use of lithium cobalt oxide (LiCoO2) enabled industrial-scale production to be achieved easily.

    This was the birth of the current lithium-ion battery.

    Then in 1991, Sony and Asahi Kasei released the first commercial lithium-ion battery.

    In 1989, Goodenough and Arumugam Manthiram of the University of Texas at Austin showed that cathodes containing polyanions, e.g. sulfates, produce higher voltages than oxides due to the inductive effect of the polyanion.[32]

    In 1996, Goodenough, Akshaya Padhi and coworkers identified lithium iron phosphate (LiFePO4) and other phospho-olivines (lithium metal phosphates with olivine structure) as cathode materials.[33]

    In 2002, Yet-Ming Chiang and his group at MIT showed a substantial improvement in the performance of lithium batteries by boosting the material's conductivity by doping it with aluminum, niobium and zirconium. The exact mechanism causing the increase became the subject of a debate.[34]

    In 2004, Chiang again increased performance by utilizing iron-phosphate particles of less than 100 nanometers in diameter. This decreased particle density by almost one hundredfold, increased the cathode's surface area and improved capacity and performance. Commercialization led to a competitive market and a patent infringement battle between Chiang and Goodenough.[34]

    [edit] Electrochemistry

    The three participants in the electrochemical reactions in a lithium-ion battery are the anode, cathode, and electrolyte.

    Both the anode and cathode are materials into which, and from which, lithium can migrate. During insertion (or intercalation) lithium moves into the electrode. During the reverse process, extraction (or deintercalation), lithium moves back out. When a lithium-based cell is discharging, the lithium is extracted from the anode and inserted into the cathode. When the cell is charging, the reverse occurs.

    Useful work can only be extracted if electrons flow through a closed external circuit. The following equations are in units of moles, making it possible to use the coefficient x.

    The positive electrode half-reaction (with charging being forwards) is: [35]



    The negative electrode half-reaction is:



    The overall reaction has its limits. Overdischarge supersaturates lithium cobalt oxide, leading to the production of lithium oxide,[36] possibly by the following irreversible reaction:



    Overcharge up to 5.2 Volts leads to the synthesis of cobalt(IV) oxide, as evidenced by x-ray diffraction[37]



    In a lithium-ion battery the lithium ions are transported to and from the cathode or anode, with the transition metal, cobalt (Co), in LixCoO2 being oxidized from Co3+ to Co4+ during charging, and reduced from Co4+ to Co3+ during discharge.

    [edit] Positive electrodes



    Electrode material

    Average potential difference

    Specific capacity

    Specific energy



    LiCoO2

    3.7 V

    140 mAh/g

    0.518 kWh/kg



    LiMn2O4

    4.0 V

    100 mAh/g

    0.400 kWh/kg



    LiNiO2

    3.5 V

    180 mAh/g

    0.630 kWh/kg



    LiFePO4

    3.3 V

    150 mAh/g

    0.495 kWh/kg



    Li2FePO4F

    3.6 V

    115 mAh/g

    0.414 kWh/kg



    LiCo1/3Ni1/3Mn1/3O2

    3.6 V

    160 mAh/g

    0.576 kWh/kg



    Li(LiaNixMnyCoz)O2

    4.2 V

    220 mAh/g

    0.920 kWh/kg


    [edit] Negative electrodes



    Electrode material

    Average potential difference

    Specific capacity

    Specific energy



    Graphite (LiC6)

    0.1-0.2 V

    372 mAh/g

    0.0372-0.0744 kWh/kg



    Hard Carbon (LiC6)

    ? V

    ? mAh/g

    ? kWh/kg



    Titanate (Li4Ti5O12)

    1-2 V

    160 mAh/g

    0.16-0.32 kWh/kg



    Si (Li4.4Si)[38]

    0.5-1 V

    4212 mAh/g

    2.106-4.212 kWh/kg



    Ge (Li4.4Ge)[39]

    0.7-1.2 V

    1624 mAh/g

    1.137-1.949 kWh/kg


    [edit] Electrolytes

    The cell voltages given in the Electrochemistry section are larger than the potential at which aqueous solutions can electrolyze, in addition lithium is highly reactive to water, therefore, nonaqueous or aprotic solutions are used.

    Liquid electrolytes in lithium-ion batteries consist of lithium salts, such as LiPF6, LiBF4 or LiClO4 in an organic solvent, such as ethylene carbonate, dimethyl carbonate, and diethyl carbonate. A liquid electrolyte conducts lithium ions, acting as a carrier between the cathode and the anode when a battery passes an electric current through an external circuit. Typical conductivities of liquid electrolyte at room temperature (20 C (68 F)) are in the range of 10 mS/cm (1 S/m), increasing by approximately 3040% at 40 C (104 F) and decreasing by a slightly smaller amount at 0 C (32 F)[40]

    Unfortunately, organic solvents easily decompose on anodes during charging. However, when appropriate organic solvents are used as the electrolyte, the solvent decomposes on initial charging and forms a solid layer called the solid electrolyte interphase (SEI),[41] which is electrically insulating yet provides sufficient ionic conductivity. The interphase prevents decomposition of the electrolyte after the second charge. For example, ethylene carbonate is decomposed at a relatively high voltage, 0.7 V vs. lithium, and forms a dense and stable interface.[citation needed]

    A good solution for the interface instability is the application of a new class of composite electrolytes based on POE (poly(oxyethylene)) developed by Syzdek et al.[42][43] It can be either solid (high molecular weight) and be applied in dry Li-polymer cells, or liquid (low molecular weight) and be applied in regular Li-ion cells.

    Another issue that Li-ion technology is facing is safety. Large scale application of Li cells in Electric Vehicles needs a dramatic decrease in the failure rate. One of the solutions is the novel technology based on reversed-phase composite electrolytes, employing porous ceramic material filled with electrolyte.[44]

    [edit] Advantages and disadvantages

    Note that both advantages and disadvantages depend on the materials and design that make up the battery. This summary reflects older designs that use carbon anode, metal oxide cathodes, and lithium salt in an organic solvent for the electrolyte.

    [edit] Advantages





    A lithium-ion battery from a laptop computer Wide variety of shapes and sizes efficiently fitting the devices they power.
    Much lighter than other energy-equivalent secondary batteries.[45]
    High open circuit voltage in comparison to aqueous batteries (such as lead acid, nickel-metal hydride and nickel-cadmium).[46] This is beneficial because it increases the amount of power that can be transferred at a lower current.
    No memory effect.
    Self-discharge rate of approximately 5-10% per month, compared to over 30% per month in common nickel metal hydride batteries, approximately 1.25% per month for Low Self-Discharge NiMH batteries and 10% per month in nickel-cadmium batteries.[47] According to one manufacturer, lithium-ion cells (and, accordingly, "dumb" lithium-ion batteries) do not have any self-discharge in the usual meaning of this word.[35] What looks like a self-discharge in these batteries is a permanent loss of capacity (see Disadvantages). On the other hand, "smart" lithium-ion batteries do self-discharge, due to the drain of the built-in voltage monitoring circuit.
    Components are environmentally safe as there is no free lithium metal.[citation needed]

    [edit] Disadvantages

    [edit] Cell life
    Charging forms deposits inside the electrolyte that inhibit ion transport. Over time, the cell's capacity diminishes. The increase in internal resistance reduces the cell's ability to deliver current. This problem is more pronounced in high-current applications. The decrease means that older batteries do not charge as much as new ones (charging time required decreases proportionally).
    High charge levels and elevated temperatures (whether from charging or ambient air) hasten capacity loss.[48][49] Charging heat is caused by the carbon anode (typically replaced with lithium titanate which drastically reduces damage from charging, including expansion and other factors).[50]
    A Standard (Cobalt) Li-ion cell that is full most of the time at 25 C (77 F) irreversibly loses approximately 20% capacity per year. Poor ventilation may increase temperatures, further shortening battery life. Loss rates vary by temperature: 6% loss at 0 C (32 F), 20% at 25 C (77 F), and 35% at 40 C (104 F). When stored at 40%60% charge level, the capacity loss is reduced to 2%, 4%, and 15%, respectively.[51][citation needed] In contrast, the calendar life of LiFePO4 cells is not affected by being kept at a high state of charge.[52]

    [edit] Internal resistance
    The internal resistance of standard (Cobalt) lithium-ion batteries is high compared to both other rechargeable chemistries such as nickel-metal hydride and nickel-cadmium, and LiFePO4 and lithium-polymer cells.[53] Internal resistance increases with both cycling and age.[49][54][55] Rising internal resistance causes the voltage at the terminals to drop under load, which reduces the maximum current draw. Eventually increasing resistance means that the battery can no longer operate for an adequate period.
    To power larger devices, such as electric cars, connecting many small batteries in a parallel circuit is more effective[56] and efficient than connecting a single large battery.[57]

    [edit] Safety requirements

    If overheated or overcharged, Li-ion batteries may suffer thermal runaway and cell rupture.[58] In extreme cases this can lead to combustion. Deep discharge may short-circuit the cell, in which case recharging would be unsafe.[59] To reduce these risks, Lithium-ion battery packs contain fail-safe circuitry that shuts down the battery when its voltage is outside the safe range of 34.2 V per cell.[35][47] When stored for long periods the small current draw of the protection circuitry itself may drain the battery below its shut down voltage; normal chargers are then ineffective. Many types of lithium-ion cell cannot be charged safely below 0C.[60]

    Other safety features are required in each cell:[35]
    shut-down separator (for overtemperature)
    tear-away tab (for internal pressure)
    vent (pressure relief)
    thermal interrupt (overcurrent/overcharging)

    These devices occupy useful space inside the cells, add additional points of failure and irreversibly disable the cell when activated. They are required because the anode produces heat during use, while the cathode may produce oxygen. These devices and improved electrode designs reduce/eliminate the risk of fire or explosion.

    These safety features increase costs compared to nickel metal hydride batteries, which require only a hydrogen/oxygen recombination device (preventing damage due to mild overcharging) and a back-up pressure valve.[47]

    [edit] Specifications and design
    Specific energy density: 150 to 250 Wh/kg (540 to 900 kJ/kg)[1]
    Volumetric energy density: 250 to 620 Wh/l (900 to 1900 J/cm)[2]
    Specific power density: 300 to 1500 W/kg (@ 20 seconds and 285 Wh/l)[1]

    Because lithium-ion batteries can have a variety of cathode and anode materials, the energy density and voltage vary accordingly.

    Lithium-ion batteries with a lithium iron phosphate cathode and graphite anode have a nominal open-circuit voltage of 3.2 V and a typical charging voltage of 3.6 V. Lithium nickel manganese cobalt (NMC) oxide cathode with graphite anodes have a 3.7 V nominal voltage with a 4.2 V max charge. The charging procedure is performed at constant voltage with current-limiting circuitry (i.e., charging with constant current until a voltage of 4.2 V is reached in the cell and continuing with a constant voltage applied until the current drops close to zero). Typically, the charge is terminated at 3% of the initial charge current. In the past, lithium-ion batteries could not be fast-charged and needed at least two hours to fully charge. Current-generation cells can be fully charged in 45 minutes or less. Some lithium-ion varieties can reach 90% in as little as 10 minutes.[61]

    [edit] Charging procedure

    Stage 1: Apply charging current until the voltage limit per cell is reached.[62]

    Stage 2: Apply maximum voltage per cell limit until the current declines below 3% of rated charge current.[62][unreliable source?]

    Stage 3: Periodically apply a top-off charge about once per 500 hours.[62][unreliable source?]

    The charge time is about three to five hours, depending on the charger used. Generally, cell phone batteries can be charged at 1C and laptop-types at 0.8C, where C is the current that would discharge the battery in one hour. Charging is usually stopped when the current goes below 0.03C but it can be left indefinitely depending on desired charging time. Some fast chargers skip stage 2 and claim the battery is ready at 70% charge.[62][unreliable source?]

    Top-off charging is recommended when voltage goes below 4.05 V/cell.[62][unreliable source?]

    Typically, lithium-ion cells are charged with 4.2 0.05 V/cell, except for military long-life cells where 3.92 V is used for extending battery life. Most protection circuits cut off if either 4.3 V or 90 C is reached. If the voltage drops below 2.50 V per cell, the battery protection circuit may also render it unchargeable with regular charging equipment. Most battery protection circuits stop at 2.73.0 V per cell.[62][unreliable source?]

    For safety reasons it is recommended the battery be kept at the manufacturer's stated voltage and current ratings during both charge and discharge cycles.

    [edit] Variations in materials and construction






    It has been suggested that Nanoball batteries be merged into this article or section. (Discuss) Proposed since September 2010.


    The increasing demand for batteries has led vendors and academics to focus on improving the power density, operating temperature, safety, durability, charging time, output power, and cost of LIB solutions.

    LIB types



    Area

    Technology

    Researchers

    Target application

    Date

    Benefit



    Cathode

    Manganese spinel (LMO)

    Lucky Goldstar Chemical,[63] NEC, Samsung,[64] Hitachi,[65] Nissan/AESC[66]

    Hybrid electric vehicle, cell phone, laptop

    1996

    durability, cost




    Lithium iron phosphate

    University of Texas/Hydro-Qubec,[67]/Phostech Lithium Inc., Valence Technology, A123Systems/MIT[68][69]

    Segway Personal Transporter, power tools, aviation products, automotive hybrid systems, PHEV conversions

    1996

    moderate density (2 Ah outputs 70 amperes) operating temperature >60 C (140 F)




    Lithium nickel manganese cobalt (NMC)

    Imara Corporation, Nissan Motor[70][71]


    2008

    density, output, safety




    LMO/NMC

    Sony, Sanyo



    power, safety (although limited durability)




    Lithium iron fluorophosphate

    University of Waterloo[72]


    2007

    durability, cost (replace Li with Na or Na/Li)




    Lithium air

    University of Dayton Research Institute[73]

    automotive

    2009

    density, safety[73]




    5% Vanadium-doped Lithium iron phosphate olivine

    Binghamton University[74]


    2008

    output



    Anode

    Lithium-titanate battery (LT)

    Altairnano

    automotive (Phoenix Motorcars), electrical grid (PJM Interconnection Regional Transmission Organization control area,[75] United States Department of Defense[76]), bus (Proterra[77])

    2008

    output, charging time, durability (20 years, 9,000 cycles), safety, operating temperature (-5070 C (-58158 F)[78][dead link]




    Lithium vanadium oxide

    Samsung/Subaru.[79]

    automotive

    2007

    density (745Wh/l)[80]




    Cobalt-oxide nano wires from genetically modified virus

    MIT


    2006

    density, thickness[81]




    Three-Dimensional (3D) Porous Particles Composed of Curved Two-Dimensional (2D) Nano-Sized Layers

    Georgia Institute of Technology [82]

    high energy batteries for electronics and electrical vehicles

    2011

    specific capacity > 2000 mAh/g, high efficiency, rapid low-cost synthesis [83]




    Iron-phosphate nano wires from genetically modified virus

    MIT


    2009

    density, thickness[84][85][86]




    Silicon/titanium dioxide composite nano wires from genetically modified tobacco virus

    University of Maryland

    explosive detection sensors, biomimetic structures, water-repellent surfaces, micro/nano scale heat pipes

    2010

    density, low charge time[87]




    Porous silicon/carbon nanocomposite spheres

    Georgia Institute of Technology

    portable electronics, electrical vehicles, electrical grid

    2010

    high stability, high capacity, low charge time[88]




    nano-sized wires on stainless steel

    Stanford University

    wireless sensors networks,

    2007

    density[89][90] (shift from anode- to cathode-limited), durability issue remains (wire cracking)




    Metal hydrides

    Laboratoire de Ractivit et de Chimie des Solides, General Motors


    2008

    density (1480 mAh/g)[91]




    Silicon Nanotubes (or Silicon Nanospheres) Confined within Rigid Carbon Outer Shells

    Georgia Institute of Technology, MSE, NanoTech Yushin's group [92]

    stable high energy batteries for cell phones, laptops, netbooks, radios, sensors and electrical vehicles

    2010

    specific capacity 2400 mAh/g, ultra-high Coulombic Efficiency and outstanding SEI stability [93]



    Electrode

    LT/LMO

    Ener1/Delphi,[94][95]


    2006

    durability, safety (limited density)




    Nanostructure

    Universit Paul Sabatier/Universit Picardie Jules Verne[96]


    2006

    density


    [edit] Usage guidelines

    [edit] Prolonging battery pack life
    Depletion below the low-voltage threshold (2.4 to 2.8 V/cell, depending on chemistry) results in a dead battery which does not even appear to charge because the protection circuit (a type of electronic fuse) disables it.[97] This can be reversed in many modern batteries, especially single-cell ones, by applying a charging voltage for long enough to make the cell voltage rise above the low-voltage threshold; however this behaviour varies by manufacturer.
    Lithium-ion batteries should be kept cool; they may be stored in a refrigerator.[97][98]
    The rate of degradation of Lithium-ion batteries is strongly temperature-dependent; they degrade much faster if stored or used at higher temperatures.[97][99]
    The rate of degradation of Lithium-ion batteries is also related to battery charge level; they degrade much faster when at 100% charge, than at lower charges. Since batteries die if deep discharged (depleted) and since a battery has some self-discharge it is frequently recommended to store batteries at 40% charge level. [100]

    [edit] Multicell devices

    Li-ion batteries require a Battery Management System to prevent operation outside each cell's Safe Operating Area (over-charge, under-charge, safe temperature range) and to balance cells to eliminate SOC mismatches, significantly improving battery efficiency and increasing overall capacity.[101] As the number of cells and load currents increase, the potential for mismatch also increases.[102] There are two kinds of mismatch in the pack: state-of-charge (SOC) and capacity/energy ("C/E") mismatch. Though SOC is more common, each problem limits pack capacity (mAh) to the capacity of the weakest cell.

    [edit] Safety

    Lithium-ion batteries can rupture, ignite, or explode when exposed to high temperature. Short-circuiting a battery will cause the cell to overheat and possibly to catch fire. Adjacent cells may also then heat up and fail, in some cases, causing the entire battery to ignite or rupture. In the event of a fire, the device may emit dense irritating smoke.[103]

    Replacing the lithium cobalt oxide cathode material in lithium-ion batteries with a lithium metal phosphate such as lithium iron phosphate, improves cycle counts, shelf life and safety, but lowers capacity. Currently, these 'safer' lithium-ion batteries are mainly used in electric cars and other large-capacity battery applications, where safety issues are critical.[104]

    Lithium-ion batteries normally contain safety devices to protect the cells from disturbance. However, contaminants inside the cells can defeat these safety devices.

    [edit] Recalls

    In March 2007, Lenovo recalled approximately 205,000 batteries at risk of explosion. In August 2007, Nokia recalled over 46 million batteries at risk of overheating and exploding.[105] One such incident occurred in the Philippines involving a Nokia N91, which uses the BL-5C battery.[106]

    In December 2006, Dell recalled approximately 22,000 laptop batteries from the U.S. market.[107] Approximately 10 million Sony batteries used in Dell, Sony, Apple, Lenovo/IBM, Panasonic, Toshiba, Hitachi, Fujitsu and Sharp laptops were recalled in 2006. The batteries were found to be susceptible to internal contamination by metal particles. Under some circumstances, these particles could pierce the separator, causing a short-circuit.[108]

    In October 2004, Kyocera Wireless recalled approximately 1 million mobile phone batteries to identify counterfeits.[109]

    [edit] Transport restrictions

    In January 2008, the United States Department of Transportation ruled that passengers on board commercial aircraft could carry lithium batteries in their checked baggage if the batteries are installed in a device. Types of batteries affected by this rule are those containing lithium, including Li-ion, lithium polymer, and lithium cobalt oxide chemistries. Lithium-ion batteries containing more than 25 grams (0.88 oz) equivalent lithium content (ELC) are exempt from the rule and are forbidden in air travel.[110] This restriction greatly reduces the chances of the batteries short-circuiting and causing a fire.[citation needed]

    Additionally, a limited number of replacement batteries may be transported in carry-on luggage. Such batteries must be sealed in their original protective packaging or in individual containers or plastic bags.[110][111]

    Some postal administrations restrict air shipping (including EMS) of lithium and lithium-ion batteries, and products containing these (e.g. laptops, cell phones etc.). Among these countries and regions are Hong Kong,[112] Australia and Japan.[113]

    [edit] Research

    Researchers are working to improve the power density, safety, recharge cycle, cost and other characteristics of these batteries.

    Solid-state designs have the potential to deliver three times the energy density of typical 2011 lithium-ion batteries at less than half the cost per kilowatt-hour. This approach eliminates binders, separators, and liquid electrolytes. By eliminating these, "you can get around 95% of the theoretical energy density of the active materials."[114]

    Earlier trials of this technology ran into cost barriers, because the semiconductor industry's vacuum deposition technology cost 2030 times too much. The new process deposits semiconductor-quality films from a solution. The nanostructured films grow directly on a substrate and then sequentially on top of each other. The process allows the firm to "spray-paint a cathode, then a separator/electrolyte, then the anode. It can be cut and stacked in various form factors."[114]

    [edit] See also





    Book: Lithium-ion batteries



    Wikipedia Books are collections of articles that can be downloaded or ordered in print.

    Potassium-ion battery
    Nanowire battery




    [edit] Notes

    1.^ a b c d "Rechargeable Li-Ion OEM Battery Products". Panasonic.com. Retrieved 2010-04-23.
    2.^ a b "Panasonic Develops New Higher-Capacity 18650 Li-Ion Cells; Application of Silicon-based Alloy in Anode". greencarcongress.com. Retrieved 2011-01-31.
    3.^ Valen & Shoesmith (2007). The effect of PHEV and HEV duty cycles on battery and battery pack performance (PDF). 2007 Plug-in Highway Electric Vehicle Conference: Proceedings. Retrieved 2010-06-11.
    4.^ 11.10V,6600Mah, Li-Ion, Replacement Laptop Battery For Dell (etc). Amazon.com Online Store. Retrieved 2010-06-11.
    5.^ H. Abea, T. Muraia and K. Zaghibb (1999). Vapor-grown carbon fiber anode for cylindrical lithium ion rechargeable batteries. Journal of Power Sources 77:2, February 1999, pp. 110-115. DOI:10.1016/S0378-7753(98)00158-X. Retrieved 2010-06-11.
    6.^ Battery Types and Characteristics for HEV ThermoAnalytics, Inc., 2007. Retrieved 2010-06-11.
    7.^ Ballon, Massie Santos (14 October 2008). "Electrovaya, Tata Motors to make electric Indica". cleantech.com. Cleantech Group. Retrieved 2010-06-11.
    8.^ [1] Monthly battery sales statistics - MoETI - March 2011
    9.^ [2] Battery Waste Management - 2006 DEFRA
    10.^ [3] EPBA statistics - 2000
    11.^ David Linden, Thomas B. Reddy (ed). Handbook Of Batteries 3rd Edition. McGraw-Hill, New York, 2002 ISBN 0-07-135978-8 chapter 35
    12.^ Silberberg, M. 2006. Chemistry: The Molecular Nature of Matter and Change, 4th Ed. New York (NY): McGraw-Hill Education. p 935.
    13.^ Thackeray, Thomas, and Whittingham (March 2000). Science and Applications of Mixed Conductors for Lithium Batteries. mrs.com; Materials Research Society. Retrieved 2010-06-11.
    14.^ MSDS: National Power Corp Lithium Ion Batteries (PDF). tek.com; Tektronix Inc., 7 May 2004. Retrieved 2010-06-11.
    15.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 2
    16.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 234
    17.^ M Stanley Whittingham. Electrical Energy Storage and Intercalation Chemistry Science: 192 (4244): 1126
    18.^ J.O.Besenhard and H.P. Fritz, Cathodic Reduction of Graphite in Organic Solutions of Alkali and NR 4+ Salts, J. Electroanal. Chem., 53, 329 (1974)
    19.^ J.O. Besenhard, The Electrochemical Preparation and Properties of Ionic Alkali Metal and NR 4+ Graphite Intercalation Compounds in Organic Electrolytes, Carbon, 14, 111 (1976)
    20.^ R. Schallhorn, R. Kuhlmann, and J.O. Besenhard, Topotactic Redox Reactions and Ion Exchange of Layered MoO3 Bronzes,, Mat. Res. Bull., 11, 83 (1976)
    21.^ J.O. Besenhard and R. Schallhorn, The Discharge Reaction Mechanism of the MoO3 Electrode in Organic Electrolytes J. Power Sources, 1, 267 (1976/77)
    22.^ J.O. Besenhard and G. Eichinger, High Energy Density Lithium Cells. Part I. Electrolytes and Anodes, J. Electroanal. Chem., 68, 1 (1976); and G. Eichinger
    23.^ J.O. Besenhard, High Energy Density Lithium Cells. Part II. Cathodes and Complete Cells, J. Electroanal. Chem., 72, 1 (1976)
    24.^ USPTO search for inventions by "Goodenough, John"
    25.^ US 4304825, Basu; Samar, "Rechargeable battery", issued 8 December 1981, assigned to Bell Telephone Laboratories
    26.^ International Meeting on Lithium Batteries, Rome, April 2729, 1982, C.L.U.P. Ed. Milan, Abstract #23
    27.^ Journal of Power Sources (AprilMay 1983), 9 (34), 365371
    28.^ M.M. Thackeray, W.I.F. David, P.G. Bruce, and J.B. Goodenough (4 February 1983). "Lithium insertion into manganese spinels". Materials Research Bulletin (Elsevier) 18 (4): 461472. doi:10.1016/0025-5408(83)90138-1.
    29.^ Gholamabbas Nazri, Gianfranco Pistoia (2004). Lithium batteries: science and ... - Google Books. Springer. ISBN 9781402076282. Retrieved 2009-10-08.
    30.^ Voelcker, John (September 2007). Lithium Batteries Take to the Road IEEE Spectrum.
    31.^ US 4668595, Yoshino; Akira, "Secondary Battery", issued 10 May 1985, assigned to Asahi Kasei
    32.^ A. Manthiram and J.B. Goodenough Corresponding (16 May 1989). "Lithium insertion into Fe2(SO4)3 frameworks". Journal of Power Sources (Elsevier B.V.) 26 (3-4): 403408. doi:10.1016/0378-7753(89)80153-3.
    33.^ "Phospho-olivines as positive-electrode materials for rechargeable lithium batteries". Electrochem. Society 144: 11881194. 1997.
    34.^ a b Editors (6 March 2008). "In search of the perfect battery" (PDF). The Economist. Archived from the original on 2009-09-25. Retrieved 2010-05-11.
    35.^ a b c d Staff (November 2003) (PDF). Lithium Ion technical handbook. Gold Peak Industries Ltd..
    36.^ H.C. Choi et al., J. Phys. Chem. B 107 p5806(2003) doi:10.1021/jp030438w
    37.^ G.G. Amatucci, J.M. Tarascon, L.C. Kein J. Electrochemical Society 143 p1114 1996 doi:10.1149/1.1836594
    38.^ R. Ruffo; S. S. Hong, C. K. Chan, R. A. Huggins, Y. Cui (2009). "Impedance Analysis of Silicon Nanowire Lithium Ion Battery Anodes" (PDF). J. Phys. Chem. C. 113 (113 (26), (2009)): 1139011398. doi:10.1021/jp901594g. Retrieved 2009-09-01.
    39.^ C. K. Chan; X. F. Zhang, Y. Cui (2007). "High Capacity Li-ion Battery Anodes Using Ge Nanowires" (PDF). Nano Lett. 8 (8 (2007)): 307309. Bibcode 2008NanoL...8..307C. doi:10.1021/nl0727157. PMID 18095738.
    40.^ Wenige, Niemann, et al. (May 30, 1998). Liquid Electrolyte Systems for Advanced Lithium Batteries (PDF). cheric.org; Chemical Engineering Research Information Center(KR). Retrieved 2010-06-11.
    41.^ Balbuena, P.B., Wang, Y.X., eds. Lithium Ion Batteries: Solid Electrolyte Interphase 2004 Imperial College Press, London
    42.^ Syzdek, Jaroslaw, et al., Journal of Power Sources, 173, 2007, p712-720 doi:10.1016/j.jpowsour.2007.05.061
    43.^ Syzdek, Jaroslaw, et al., Electrochimica Acta, 55, 2010, p1314-1322, doi:10.1016/j.electacta.2009.04.025
    44.^ Syzdek, Jaroslaw, et al., Journal of Power Sources, 194, 2009, p66-72, doi:10.1016/j.jpowsour.2009.01.070
    45.^ Winter & Brodd 2004, pp. 4256, 4258
    46.^ , Winter & Brodd 2004, p. 4254
    47.^ a b c Winter & Brodd 2004, p. 4259
    48.^ Aging - capacity loss BatteryUniversity.com.[unreliable source?]
    49.^ a b Winter & Brodd 2004, p. 4258
    50.^ Altair Nano: Power & Energy Systems[dead link]
    51.^ . Battery University: Fig. 1 Non-recoverable capacity loss[unreliable source?]
    52.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 9
    53.^ "A123 M1 cell specifications".
    54.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 12
    55.^ Buchmann, Isidor (200804). "Choosing a battery that will last". Isidor Buchmann (CEO of Cadex Electronics Inc.).[unreliable source?]
    56.^ Battery Management Systems for Large Lithium-Ion Battery Packs page 229
    57.^ Buchmann, Isidor (September 2006). "BatteryUniversity.com: How to prolong lithium-based batteries". Cadex Electronics Inc..[unreliable source?]
    58.^ Spotnitz, R.; Franklin, J. (2003). "Abuse behavior of high-power, lithium-ion cells". Journal of Power Sources (Elsevier) 113: 81100. doi:10.1016/S0378-7753(02)00488-3.
    59.^ Buchmann, Isidor (February 2003). "Advanced battery analyzers". Isidor Buchmann. Retrieved 2009-12-26.[unreliable source?]
    60.^ "Lithium-ion Battery Charging Basics". PowerStream Technologies. Retrieved 4 December 2010.
    61.^ AeroVironment achieves electric vehicle fast-charge milestone avinc.com; AeroVironment, 30 May 2007. (Press release). "Test rapidly recharges a battery pack designed for use in passenger vehicles. 10-minute recharge restores enough energy to run electric vehicle for two hours at 60 miles per hour."
    62.^ a b c d e f "Charging lithium-ion batteries". batteryuniversity.com. Retrieved 2009-05-21.[unreliable source?]
    63.^ Kevin Jost [ed.] (October 2006). Tech Briefs: CPI takes new direction on Li-ion batteries (PDF). aeionline.org; Automotive Engineering Online. Archived from the original. Retrieved 2010-06-11.
    64.^ Voelcker, John (September 2007). Lithium Batteries Take to the Road. IEEE Spectrum. Retrieved 2010-06-15.
    65.^ Loveday, Eric (23 April 2010). "Hitachi develops new manganese cathode, could double life of li-ion batteries". Retrieved 2010-06-11..
    66.^ Nikkei (29 November 2009). Report: Nissan On Track with Nickel Manganese Cobalt Li-ion Cell for Deployment in 2015 Green Car Congress (blog). Retrieved 2010-06-11.
    67.^ Elder, Robert and Zehr, Dan (16 February 2006). Valence sued over UT patent Austin American-Statesman (courtesy Bickle & Brewer Law Firm). Archived from the original. Retrieved 2010-06-11.
    68.^ Bulkeley, William M. (26 November 2005). "New Type of Battery Offers Voltage Aplenty, at a Premium". The Day: p. E6.
    69.^ A123Systems (2 November 2005). A123Systems Launches New Higher-Power, Faster Recharging Li-Ion Battery Systems Green Car Congress; A123Systems (Press release). Retrieved 2010-05-11.
    70.^ Imara Corporation website
    71.^ O'Dell, John (17 December 2008). Fledgling Battery Company Says Its Technology Boosts Hybrid Battery Performance Green Car Advisor; Edmunds Inc. Retrieved 2010-06-11.
    72.^ B. L. Ellis, W. R. M. Makahnouk, Y. Makimura, K. Toghill & L. F. Nazar (9 September 2007). A multifunctional 3.5 V iron-based phosphate cathode for rechargeable batteries. 6. Nature Materials. pp. 749753. Bibcode 2007NatMa...6..749E. doi:10.1038/nmat2007. Retrieved 2009-10-08.
    73.^ a b "A Research First: Lithium Air Battery Development (Press Release)". 17 November 2009. Retrieved 2010-06-11.
    74.^ Jian Hong, C. S. Wang, Shailesh Upreti and M. Stanley Whittinghama. "Vanadium Modified LiFePO4 Cathode for Li-ion Batteries". ECS (ETS) 12 (2): A33. Retrieved 2010-06-11.
    75.^ Altair Nanotechnologies (21 November 2008). "... Acceptance of the First Grid-Scale, Battery Energy Storage System". Press release. Retrieved 2009-10-08.
    76.^ Marty Ozols (11 November 2009). Altair Nanotechnologies Power Partner - The Military Systemagicmotives (personal webpage)[dubious discuss]. Retrieved 2010-06-11.
    77.^ "Proterra Corporate website". Proterra. Retrieved 2009-10-08.[dead link]
    78.^ Microsoft PowerPoint - 061125 Altair EDTA Presentation
    79.^ Blain, Loz (2 November 2007). "Subaru doubles the battery range on its electric car concept". gizmag. Retrieved 2009-10-08.
    80.^ "Li-Ion Rechargeable Batteries Made Safer". Nikkei Electronics Asia. 29 January 2008. Retrieved 2009-10-08.
    81.^ Ki Tae Nam, Dong-Wan Kim, et. al. (6 April 2006). Virus-Enabled Synthesis and Assembly of Nanowires for Lithium Ion Battery Electrodes. Science Express (preprint). Retrieved 2010-06-11.(subscription required)
    82.^ "gatech.edu".
    83.^ Kara Evanoff, Alexandre Magasinskiy, Junbing Yang and Gleb Yushin (April 21, 2011). "Nanosilicon-Coated Graphene Granules as Anodes for Li-Ion Batteries". Advanced Energy Materials. doi:10.1002/aenm.201100071. Retrieved 2011-04-21.
    84.^ Palca, Joe (6 April 2009). Hidden Ingredient In New, Greener Battery: A Virus. npr.org; National Public Radio. Retrieved 2010-06-11.
    85.^ Zandonella, Catherine (11 April 2009). "Battery grown from "armour plated" viruses". New Scientist (Tribune media Services International) 202 (2703): 1.
    86.^ Bullis, Kevin (28 September 2006). "Powerful Batteries That Assemble Themselves". technologyreview.com. Technology Review. Retrieved 2010-06-15.
    87.^ "Bad Virus Put to Good Use". Clark School of Engineering, University of Maryland. December 6, 2010. Retrieved December, 2010.
    88.^ "Self-Assembled Nanocomposites Boost Lithium-Ion Battery Anodes". Nature Materials and Georgia Institute of Technology. March 15, 2010. Retrieved March, 2010.
    89.^ "New Nanowire Battery Holds 10 Times The Charge Of Existing Ones". sciencedaily.com. Science Daily. 20 December 2007.
    90.^ Dennis, Lyle (21 December 2007). "Interview with Dr. Cui, Inventor of Silicon Nanowire Lithium-ion Battery Breakthrough". GM-Volt. Retrieved 2009-10-08.
    91.^ Y. Oumellal, A. Rougier, G. A. Nazri, J-M. Tarascon & L. Aymard (12 October 2008). "Metal hydrides for lithium-ion batteries". Nature Materials 7 (11): 916921. Bibcode 2008NatMa...7..916O. doi:10.1038/nmat2288. Retrieved 2009-10-08.
    92.^ "Error: no |title= specified when using {{Cite web}}". http://www.nano-tech.gatech.edu/.
    93.^ Benjamin Hertzberg, Alexander Alexeev and Gleb Yushin (June 8, 2010). "Deformations in Si?Li Anodes Upon Electrochemical Alloying in Nano-Confined Space". JACS 132 (25): 85488549. doi:10.1021/ja1031997. Retrieved 2010-06-08.
    94.^ Welcome to Ener1. Ener1 (Press release). Archived from the original 2006-07-08. Retrieved 2010-06-11.
    95.^ EnerDel Technical Presentation (PDF). EnerDel Corporation. 29 October 2007. Archived from the original. Retrieved 2010-06-11.
    96.^ Bullis, Kevin (22 June 2006). Higher-Capacity Lithium-Ion Batteries Technology Review. Retrieved 2010-06-11.
    97.^ a b c http://batteryuniversity.com/parttwo-34.htm
    98.^ L.M. Cristo, T. B. Atwater. Characteristics and Behavior of 1M LiPF6 1EC:1DMC Electrolyte at Low Temperatures. Fort Monmouth, NJ: U.S. Army Research.
    99.^ Modelling capacity fade in Lithium-ion cells, Bor Yann Liaw, Jungst, Nagasubramanian, and Doughty, Sandia National Laboratory
    100.^ batteryuniversity.com: How to Prolong Lithium-based Batteries, Research is performed by the Center for Automotive Research at the Ohio State University in collaboration with Oak Ridge National Laboratory and the National Institute of Standards Technology
    101.^ Andrea, Davide (21 August 2008). About Battery Management Systems. ELithion LLC. Retrieved 2010-06-15.
    102.^ Andrea, Davide (19 September 2008). White Paper - CCCV chargers: a false sense of security. ELithion LLC. Retrieved 2010-06-15.
    103.^ Electrochem Commercial Power (9 September 2006). "Safety and handling guidelines for Electrochem Lithium Batteries" (PDF). http://marine.rutgers.edu. Rutgers University. Retrieved 2009-05-21.
    104.^ Cringely, Robert X. (1 September 2006). "Safety Last". The New York Times. Retrieved 2010-04-14.
    105.^ Nokia issues BL-5C battery warning, offers replacement. Wikinews. 14 August 2007. Retrieved 2009-10-08.
    106.^ Staff (27 July 2007). Nokia N91 cell phone explodes Mukamo - Filipino News (blog). Retrieved 2010-06-15.
    107.^ Tullo, Alex. (21 August 2006). "Dell Recalls Lithium Batteries". Chemical and Engineering News:11; American Chemical Society. Retrieved 2010-06-15.
    108.^ Hales, Paul (21 June 2006). Dell laptop explodes at Japanese conference. The Inquirer. Retrieved 2010-06-15.
    109.^ Kyocera Wireless (28 October 2004). "Kyocera Launches Precautionary Battery Recall, Pursues Supplier of Counterfeit Batteries". Press release. Archived from the original on 7 January 2006. Retrieved 2010-06-15.
    110.^ a b "Safe Travel". Safetravel.dot.gov. U.S. Department of Transportation. 1 January 2008. Retrieved 2009-10-08.
    111.^ Galbraith, Rob (3 January 2008). "U.S. Department of Transportation revises lithium battery rules press release". Little Guy Media. Retrieved 2009-05-11.
    112.^ Prohibitions - 6.3.12 - Dangerous, offensive and indecent articles (PDF). Hong Kong Post Office Guide. December 2009. Retrieved 2010-06-15.
    113.^ International Mail > FAQs > Goods/Services: Shipping a Laptop Japan Post Service Co. Ltd. Retrieved 2010-06-15.
    114.^ a b Melody Voth (December 6, 2010). "Battery Booster". Retrieved February 9, 2011.

    [edit] References

    Winter, M.; Brodd, J. (2004). "What Are Batteries, Fuel Cells, and Supercapacitors?" (PDF). Chemical Review 104 (104): 4245. doi:10.1021/cr020730k. Retrieved 2010-07-25.

    [edit] External links





    Wikimedia Commons has media related to: Lithium-ion batteries

    Asahi Kasei Corporation -- Father of the lithium-ion battery
    Lithium batteries at the Open Directory Project
    Argonne opens chapter in battery research -- lithium air. Argonne National Labs. Press release. 14 September 2009.
    Battery and Energy Technologies - Rechargeable Lithium batteries. Electropaedia; Woodbank Communications Ltd. Updated 28 April 2010.
    Stanford's nanowire battery holds 10 times the charge of existing ones. Stanford Report, 18 December 2007. Press release.
    The Lithium Ion Battery. E-Articles.com. (Self-publishing site).
    The Future of Electric Vehicles: Setting the Record Straight on Lithium Availability. Journal of Energy Security, 27 August 2009. Keith Evans.
    Researchers from Spheric Technologies and Arizona State University Describe Major Advances in the Use of Microwaves to Produce Key Lithium Ion Battery Materials; Present Papers at MS&T'10 Conference, October 17-21. Spheric Technologies. Press release. October 18, 2010.






    [hide]v d eGalvanic cells






    Non-rechargeable:
    primary cells


    Alkaline battery Aluminium battery Bunsen cell Chromic acid cell Clark cell Daniell cell Dry cell Grove cell Leclanch cell Lithium battery Mercury battery Nickel oxyhydroxide battery Silver-oxide battery Weston cell Zamboni pile Zincair battery Zinccarbon battery Zincchloride battery








    Rechargeable:
    secondary cells


    Automotive battery Leadacid battery Lead-acid battery (gel) Lithium air battery Lithium-ion battery Beltway battery Lithium-ion polymer battery Lithium iron phosphate battery Lithium sulfur battery Lithium-titanate battery Nickel-cadmium battery Nickel hydrogen battery Nickel-iron battery Nickel-lithium battery Nickel-metal hydride battery Low self-discharge NiMH battery Nickel-zinc battery Potassium-ion battery Rechargeable alkaline battery Silicon air battery Sodium-ion battery Sodium-sulfur battery Vanadium redox battery Zinc-bromine battery Zinc-cerium battery






    Kinds of cells


    Battery (including Wet cell Dry cell) Concentration cell Flow battery Fuel cell Trough battery Voltaic pile






    Parts of cells


    Anode Catalyst Cathode Electrolyte Half cell Ions Salt bridge Semipermeable membrane








    View page ratings



    Rate this page



    What's this?






    Trustworthy
















    Objective
















    Complete
















    Well-written

















    I am highly knowledgeable about this topic (optional)












    Submit ratings













































    Categories: Lithium-ion batteries | Rechargeable batteries | Metal-ion batteries | Product recalls | Product safety scandals







    Log in / create account




    Article
    Discussion








    Read
    Edit
    View history

















    Main page
    Contents
    Featured content
    Current events
    Random article
    Donate to Wikipedia


    Interaction

    Help
    About Wikipedia
    Community portal
    Recent changes
    Contact Wikipedia


    Toolbox










    Print/export






    Languages

    ???????
    ?????????
    Catal
    ?esky
    Dansk
    Deutsch
    Eesti
    Espaol
    Esperanto
    ?????
    Franais
    ???
    Italiano
    Magyar
    ??????
    Nederlands
    ???
    ?Norsk (bokml)?
    Polski
    Portugus
    Romn?
    ???????
    Simple English
    Suomi
    Svenska
    Trke
    ??????????
    ??

    This page was last modified on 27 July 2011 at 11:51.

    Text is available under the Creative Commons Attribution-ShareAlike License; additional terms may apply. See Terms of use for details.
    Wikipedia is a registered trademark of the Wikimedia Foundation, Inc., a non-profit organization.

    Contact us
    Privacy policy
    About Wikipedia
    Disclaimers





  8. #17
    Guest

    The right thing??The carbon

    The right thing??The carbon footprint for electric vehicles is larger than for gasoline fired vehicles.
    20k to replace the battery at 8 yrs. Contiual voltage depletion over time. After 6 yrs the vehicle will have zero value.

    ijv5x

  9. #18
    Guest

    We almost always get 300,000

    We almost always get 300,000 miles to our hondas, doges, and mazdas we've had. Then take them to the junk yard to get $1000 dollars.

  10. #19
    Guest

    I have a 95 Honda Civic (

    I have a 95 Honda Civic ( which I love love love) has 189,000 and have never had an issue with anything. I am in the market for a used hybrid now, but am nervous about getting stuck with one that will soon need a battery replacement. Battery advice anyone? Is it enevitable that all hybrid vehicles will eventually need new batteries, or does this only happen because the vehicle is poorly cared for?

  11. #20
    Guest

    Riley.You mention that your

    Riley.You mention that your IMA light is on but wont that cause you check engine light to come on ? and wont that cause you to fail your inspection. I also have a IMA light on @ 175400 and it wont pass inspection in NY. It seem to run great but I wont be able to drive it any longer without spending big bucks to get it repaired. Any suggerstions ouy there.

    Paul from western NY

Posting Permissions

  • You may not post new threads
  • You may not post replies
  • You may not post attachments
  • You may not edit your posts